Journal Articles
Alloy Digest (1968) 17 (7): Al-177.
Published: 01 July 1968
... APEX 85 is beat treatable aluminum sand and permanent mold casting alloy. It is recommended for applications where good high temperature strength, high hardness, resistance to wear and good machinability are required. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1987) 36 (4): Al-279.
Published: 01 April 1987
... APEX TERNALLOY 7 is one of a family of three APEX TERNALLOYS; see also APEX TERNALLOY 5 (Alloy Digest A1-273, revised March 1987) and APEX TERNALLOY 6 (Alloy Digest A1-277, February 1987). It can be hardened by aging at room temperature without a solution treatment and offers high mechanical...
Journal Articles
Alloy Digest (1956) 5 (3): Al-37.
Published: 01 March 1956
... APEX Z-50 is a heat treatable aluminum casting alloy suitable for sand and permanent mold castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1963) 12 (2): Al-122.
Published: 01 February 1963
... APEX Z39-11 is an aluminum die casting alloy containing copper, silicon and zinc. It is a modification of Apex 39-11 by the addition of zinc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture...
Journal Articles
Alloy Digest (1987) 36 (2): Al-277.
Published: 01 February 1987
... APEX TERNALLOY 6 is one of a family of three APEX aluminum casting alloys (See APEX TERNALLOY 5, A1-273, November 1986.). It can be hardened by aging at room temperature and offers high mechanical properties. It has good castability, excellent machinability and high resistance to corrosion. Its...
Journal Articles
Alloy Digest (1961) 10 (2): Al-100.
Published: 01 February 1961
... APEX 39-11 is an aluminum die casting alloy containing copper and silicon. It has excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1959) 8 (8): Al-81.
Published: 01 August 1959
... and machining. Filing Code: Al-81. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International chemical composition elasticity hardness heat treatability high-temperature alloys machinability physical...
Journal Articles
Alloy Digest (1962) 11 (6): Al-8.
Published: 01 June 1962
... on heat treating, machining, and joining. Filing Code: Al-8. Producer or source: Apex Smelting Company. Originally published July 1953, revised June 1962. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International ALLCAST 60 chemical composition...
Journal Articles
Alloy Digest (1957) 6 (11): Al-59.
Published: 01 November 1957
... treating, machining, and joining. Filing Code: Al-59. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International castability chemical composition corrosion-resistant alloys elasticity hardness heat...
Journal Articles
Alloy Digest (1960) 9 (2): Al-89.
Published: 01 February 1960
... temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-89. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International castability chemical...
Journal Articles
Alloy Digest (1959) 8 (11): Al-86.
Published: 01 November 1959
... as heat treating, machining, and joining. Filing Code: Al-86. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat...
Journal Articles
Alloy Digest (1952) 1 (1): Al-1.
Published: 01 September 1952
...: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International castability chemical composition corrosion-resistant alloys hardness heat treatability joinability machinability physical properties sand castings tensile...
Journal Articles
Alloy Digest (1968) 17 (5): Al-175.
Published: 01 May 1968
..., and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Al-175. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996...
Journal Articles
Alloy Digest (1973) 22 (4): TS-253.
Published: 01 April 1973
..., and fused-to-steel rods. Applications: Cold and warm heading, warm forming, impact extrusion, rotary swaging, rotary combustion-engine apex strips, heavy cold forming, heavy piercing, hobs and reamers for nonferrous metals, jet fuel-pump rotors and vanes, and hot aluminum extrusion. Manufacturer: Chromalloy...