1-20 of 21 Search Results for

Apex 400

Sort by
Journal Articles
Alloy Digest (1961) 10 (9): Al-107.
Published: 01 September 1961
... APEX 400 is a 4% magnesium type aluminum casting alloy having high corrosion resistance. It is not heat treatable. It is recommended for marine applications and food processing equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1964) 13 (5): Al-137.
Published: 01 May 1964
... APEX 28 is an aluminum-copper-silicon die casting alloy recommended for intricate and thin wall sections. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also...
Journal Articles
Alloy Digest (1963) 12 (2): Al-122.
Published: 01 February 1963
... APEX Z39-11 is an aluminum die casting alloy containing copper, silicon and zinc. It is a modification of Apex 39-11 by the addition of zinc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture...
Journal Articles
Alloy Digest (1967) 16 (5): Al-166.
Published: 01 May 1967
... TENSILE PROPERTIES AT ELEVATED TEMPERATURES (Apex 12) (Lowest strengths during 10,000 hours of heating at test temperatures) Test Tensile Yield Temperature Strength Strength Elongation F psi psi (0.2%) % in 2 75 23000 15000 1.5 212 22500 14000 1.5 300 22000 13000 1.5 400 21000 12000 5 14 0 600 6000 4000...
Journal Articles
Alloy Digest (1961) 10 (2): Al-100.
Published: 01 February 1961
... APEX 39-11 is an aluminum die casting alloy containing copper and silicon. It has excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1958) 7 (6): Al-66.
Published: 01 June 1958
... APEX 36 is a high silicon, aluminum die casting alloy having high fluidity, excellent castability and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness...
Journal Articles
Alloy Digest (1968) 17 (7): Al-177.
Published: 01 July 1968
... APEX 85 is beat treatable aluminum sand and permanent mold casting alloy. It is recommended for applications where good high temperature strength, high hardness, resistance to wear and good machinability are required. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1958) 7 (10): Al-71.
Published: 01 October 1958
... APEX Z39 is an aluminum-copper-silicon-zinc die casting alloy having excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes...
Journal Articles
Alloy Digest (1959) 8 (1): Al-75.
Published: 01 January 1959
... APEX 39 is an aluminum die casting alloy ingot containing copper and silicon. It has excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1957) 6 (8): Al-54.
Published: 01 August 1957
... APEX 418 is an aluminum die casting alloy having excellent combination of high strength and corrosion resistance, also high ductility and finishing qualities. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1956) 5 (10): Mg-28.
Published: 01 October 1956
... APEX 910 is a magnesium die casting alloy containing about 9% aluminum. It combines good mechanical properties, good casting characteristics, and good resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1956) 5 (3): Al-37.
Published: 01 March 1956
... APEX Z-50 is a heat treatable aluminum casting alloy suitable for sand and permanent mold castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1960) 9 (2): Al-89.
Published: 01 February 1960
... temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-89. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International castability chemical...
Journal Articles
Alloy Digest (1959) 8 (11): Al-86.
Published: 01 November 1959
... as heat treating, machining, and joining. Filing Code: Al-86. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity hardness heat...
Journal Articles
Alloy Digest (1959) 8 (8): Al-81.
Published: 01 August 1959
... and machining. Filing Code: Al-81. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International chemical composition elasticity hardness heat treatability high-temperature alloys machinability physical...
Journal Articles
Alloy Digest (1962) 11 (6): Al-8.
Published: 01 June 1962
... on heat treating, machining, and joining. Filing Code: Al-8. Producer or source: Apex Smelting Company. Originally published July 1953, revised June 1962. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996 1996 ASM International ALLCAST 60 chemical composition...
Journal Articles
Alloy Digest (1968) 17 (5): Al-175.
Published: 01 May 1968
..., and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Al-175. Producer or source: Apex Smelting Company. Producer or Source: Apex Smelting Company Copyright © ASM International® 1996...
Journal Articles
Alloy Digest (1966) 15 (8): Al-14.
Published: 01 August 1966
..., crankcases. Commonly used for parrs requiring strength and ruggedness. Manufacturers: Niagara Falls Smelting and Refining Co.. Buffalo, New York. Aluminum Company of America, Pittsburgh, Pennsylvania. Kaiser Aluminum and Chemical Corp., Oakland, California. Reynols Metals Company, Louisville, Kentucky. Apex...
Journal Articles
Alloy Digest (1973) 22 (4): TS-253.
Published: 01 April 1973
..., and fused-to-steel rods. Applications: Cold and warm heading, warm forming, impact extrusion, rotary swaging, rotary combustion-engine apex strips, heavy cold forming, heavy piercing, hobs and reamers for nonferrous metals, jet fuel-pump rotors and vanes, and hot aluminum extrusion. Manufacturer: Chromalloy...
Journal Articles
Alloy Digest (1954) 3 (7): Al-18.
Published: 01 July 1954
..., and for sound and pressure tight cast- he Manufacturer: Reynolds Metals Company, Louisville, Kentucky Aluminum Company of America, Pittsburgh, Pennsylvania Kaiser Ahlminum % chemical Saks Corp., oaklan& caLfomia Apex Smelting Company, Cleveland, Ohio & Chicago, Uinois 1Or DIGEST CARPENTER No. 5-876 RltgcokfA-8...