Journal Articles
Alloy Digest (2013) 62 (3): Cu-816.
Published: 01 March 2013
... Ansonia alloys C64200 and C64210 are aluminum bronze alloys with great machinability for alloys without lead. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining...