Alloy Digest (2008) 57 (8): Cu-757.
Published: 01 August 2008
... Ansonia alloy C54400, a leaded phosphor bronze alloy, combines machinability with bearing properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining...