Alloy Digest (2015) 64 (11): CS-193.
Published: 01 November 2015
... Ancorsteel FLD-49DH is a nickel-free copper-molybdenum alloy steel powder developed for sinter-hardening applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on powder...