Alloy Digest (2012) 61 (9): CS-170.
Published: 01 September 2012
... Ancorsteel AMH alloy is a low apparent density, water-atomized alloy for structural applications. This datasheet provides information on composition and physical properties. It also includes information on powder metal forms. Filing Code: CS-170. Producer or source: Hoeganaes Corporation...