Alloy Digest (2013) 62 (4): SA-676.
Published: 01 April 2013
... Ancorloy HP-1 is a press-ready, engineered binder-treated premixed ferrous powder metallurgy material designed for enhanced as-sintered mechanical properties. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (2010) 59 (12): SA-619.
Published: 01 December 2010
... Ancorloy DH-1 is a hybrid alloy based on Ancorsteel 150 HP (Alloy Digest CS-154, July 2010) to which 2% w/o copper has been added. In the powder production process used to make Ancorsteel, molten steel is atomized into irregular, homogeneous particles which are then annealed to produce uniform...