1-1 of 1 Search Results for

AncorLam

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2016) 65 (1): CS-194.
Published: 01 January 2016
... AncorLam is a high performance insulated particle material suitable for a variety of soft magnetic applications that require low core losses. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on powder metal forms. Filing...