1-6 of 6 Search Results for

Ampcoloy 95

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (10): Cu-789.
Published: 01 October 2010
... Ampcoloy 95 has slightly higher mechanical properties than most alloys in its class. Applications include spot welding electrodes. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming and machining...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (9): Cu-787.
Published: 01 September 2010
... CrMo4) 250 max 100 AMPCO 8 109 124 125 AMPCO 18 159 183 130 AMPCO M4 270 305 120 AMPCO 21 285 311 115 AMPCO 22 321 352 110 AMPCO 25 356 394 100 AMPCO 26 395 450 75 Ampcoloy 940, 95, 972 180 255 125 Ampcoloy 83 340 390 100 Ampcoloy 88 260 280 120 General Characteristics: Ampcoloy 88 was originated...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1976) 25 (3): Cu-310.
Published: 01 March 1976
... AMPCOLOY 83 is a wrought copper-base alloy containing nominally 1.8% beryllium. It offers good formability in the unhardened condition and can be strengthened by precipitation hardening. It has a combination of high strength and hardness, good ductility, good electrical and thermal conductivity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1978) 27 (12): Cu-363.
Published: 01 December 1978
... with standard silver alloy filler metals. In soldering, best results are obtained by using 50-50 lead-tin or 95-5 tin-antimony solders and an acid flux. Corrosion Resistance: Ampcoloy 522 is outstanding up to 7000F in its resistance to general and impingement attack by clean sea water; at low water velocities...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (12): Cu-408.
Published: 01 December 1980
... be either argon or helium. Excellent results can be obtained by brazing with standard silver alloy filler metals. In soldering, good results are obtained by using 50 lead-50 tin or 95 tin-5 antimony solders and an acid flux. Corrosion Resistance: Ampcoloy 521 is outstanding in its resistance to general...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (12): Cu-793.
Published: 01 December 2010
... www.ampcometal.com Ampcoloy is a registered trademark of Ampco Metal SA. Table 1 Mechanical properties Property Nominal values Ultimate tensile strength, MPa (ksi) 758 (110) Yield strength, RP 0.5, MPa (ksi) 386 (56) Elongation 2 in., % 16 Brinell hardness, HB 30 207 Rockwell hardness, HRB 95 Reduction of area, % 16...