Alloy Digest (1991) 40 (10): Al-320.
Published: 01 October 1991
... performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-320. Producer or source: Various aluminum companies. Producer or Source: Various aluminum companies Copyright © ASM International® 1996 1996 ASM International Aluminum alloys 6063...
Journal Articles
Alloy Digest (1974) 23 (1): Al-42.
Published: 01 January 1974
... ALUMINUM 6063 is an age-hardenable extrusion alloy with excellent working properties especially in the annealed condition. It has excellent resistance to corrosion in all tempers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (2005) 54 (4): Al-392.
Published: 01 April 2005
... Code: Al-392 Aluminum April 2005 ALCOA 6063 (Extruded Aluminum Alloy) Alloy 6063, one of the most popular alloys in the 6000 series, provides good extrudability and a high-quality surface finish. Alloy 6063 is used in a variety of architectural applications. Table 1 Mechanical and Physical Property...
Journal Articles
Alloy Digest (1968) 17 (3): Al-173.
Published: 01 March 1968
... Aluminum 6563 is an aluminum extrusion alloy recommended for trim applications, combining medium strength and formability with good finishing characteristics. It responds to an age-hardening heat treatment. Alloy 6563 is a modification of alloy 6063 with improved finishing characteristics...
Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
... 2019. Producer or Source: Kaiser Aluminum Copyright © ASM International® 2011 2011 ASM International chemical composition corrosion-resistant alloys elasticity fatigue properties hardness heat treatability joinability KAISER ALLOY 6063 physical properties shear strength tensile...
Journal Articles
Alloy Digest (2019) 68 (7): Al-458.
Published: 01 July 2019
...), 10 6/K (10 6/°F) 23.4 (13.0) Copyright © 2019, ASM International®. All rights reserved. KAISER ALLOY 6063 (High-Strength Alloy) Filing Code: Al-458 Aluminum :: July 2019 Materials Park, Ohio 44073-0002 :: 440.338.5151 :: Fax 440.338.4634 :: www.asminternational.org :: MemberServiceCenter...
Journal Articles
Alloy Digest (2022) 71 (7): Al-488.
Published: 01 July 2022
... Atlas 6063 is a wrought, heat-treatable, aluminum-magnesium-silicon extrusion alloy (6xxx series) that offers good mechanical properties. It responds well to polishing, chemical brightening, anodizing, and dyeing. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1998) 47 (9): Al-353.
Published: 01 September 1998
... characterization by temper General Characteristics: Alloy C238 is a moderate-strength aluminum screw machine stock alloy. Its main attributes are superior postbrazing and welding strength. It has good machinability as compared to 6061 and 6063 alloys. The product is also available in cold- heading rod...
Journal Articles
Alloy Digest (2005) 54 (5): Al-393.
Published: 01 May 2005
... Alloys 6605 and 6105 belong to the 6xxx series of aluminum alloys. They are medium strength alloys and are used as structural members such as handrails and ladders. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes...
Journal Articles
Alloy Digest (2002) 51 (8): Al-380.
Published: 01 August 2002
... 4.5 6.0 Iron 0.8 max Copper 0.30 max Manganese 0.05 max Magnesium 0.05 max Zinc 0.15 max Titanium 0.20 max Beryllium 0.0008 max Others, each 0.05 max Others, total 0.15 max Aluminum bal Physical Properties: Density, kg/m3 (lb/in.3 ) 2685 (0.097) Conductivity, O temper, %IACS 42 Melting range, °C (°F...
Journal Articles
Alloy Digest (2005) 54 (8): Al-396.
Published: 01 August 2005
... 2005 ALCOA 6101 (Extruded Aluminum Alloy) Alloy 6101 is an age-hardenable alloy for applications requiring both moderate strength and maximum electrical resistivity. Table 1 Mechanical and Physical Property Limits Yield strength, Thermal conductivity at Electrical Specified section or wall thickness...
Journal Articles
Alloy Digest (2002) 51 (3): Al-324.
Published: 01 March 2002
... Characteristics: Filler wire 4643 was developed by taking the well-known alloy 4043, reducing the silicon content, and adding 0.10 0.30% Mg. This combination introduces Mg2Si into the weld puddle, which responds to the postweld heat treatment and aging required to obtain properties in the 6xxx family of aluminum...
Journal Articles
Alloy Digest (1969) 18 (2): Al-184.
Published: 01 February 1969
..., does not show the type of internal shrinkage characteristic of other aluminum alloys with smaller solidification range. Alloy 4043 is recommended as a filler metal when resistance to salt water corrosion is required, especially when welding such aluminum alloys as 5052, 6061 and 6063. It is recommended...
Journal Articles
Alloy Digest (1998) 47 (6): Al-349.
Published: 01 June 1998
...~. All bghts reserved. Data shown are t@cat, not to be used forspedfication or finat design. 1 *tGIM%%fkD 1 DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: Aluminum Al-349 June 1998 Puhtdhed b)c ASM Intematkmat Matedats Park. Ohio 440734002 440-333-5151 Fax44@3384634 Mem-ServOpo.ASh4-lnil.oq ALCOA 6061...
Journal Articles
Alloy Digest (2002) 51 (9): Al-381.
Published: 01 September 2002
... properties Chemical Composition, wt Silicon 11.0 13.0 Iron 0.8 max Copper 0.30 max Manganese 0.15 max Magnesium 0.10 max Zinc 0.20 max Beryllium 0.0008 max Others, each 0.05 max Others, total 0.15 max Aluminum bal Physical Properties: Density, kg/m3 (lb/in.3 ) 2657 (0.096) Electrical conductivity, 41 O...
Journal Articles
Alloy Digest (1973) 22 (6): Al-39.
Published: 01 June 1973
... ALUMINUM 5052 is nominally an aluminum-magnesium-chromium alloy which cannot be hardened by heat treatment; however, it can be strain hardened by cold working. It combines good workability with good fatigue strength and high corrosion resistance to the atomsphere and to salt water. This datasheet...
Journal Articles
Alloy Digest (1973) 22 (12): Al-31.
Published: 01 December 1973
... ALUMINUM 3003 is a wrought non-heat-treatable aluminum alloy with excellent resistance to corrosion. It is used widely in deep-drawing and forming applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (2016) 65 (8): Al-445.
Published: 01 August 2016
... Alcotec weld filler wire 5356 is a non-heat-treatable aluminum welding wire whose principal alloying elements are magnesium, manganese, and chromium. It is similar to the European wire AlMg5Cr(A). This datasheet provides information on composition, physical properties, and tensile properties...
Journal Articles
Alloy Digest (2022) 71 (8): Al-489.
Published: 01 August 2022
... Austral Wright 5005 is a wrought, non-heat-treatable, aluminum-magnesium alloy (5xxx series) that exhibits moderate strength, good formability, and good resistance to corrosion in marine atmospheres. It is widely used for decorative and architectural applications. This datasheet provides...
Journal Articles
Alloy Digest (2002) 51 (4): Al-376.
Published: 01 April 2002
... Wire Corporation. Producer or Source: AlcoTec Wire Corporation Copyright © ASM International® 2002 2002 ASM International ALCOTEC WELD WIRE 5356 chemical composition joinability physical properties shear strength tensile properties wires wrought aluminum alloys thermal properties...