Skip Nav Destination
Close Modal
Search Results for
Aluminum alloys 5657
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-3 of 3 Search Results for
Aluminum alloys 5657
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1991) 40 (6): Al-317.
Published: 01 June 1991
... AA 5657 is a binary aluminum/magnesium alloy of moderate strength. It is not hardenable by heat treatment. It is strain hardenable. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information...
Abstract
View article
PDF
AA 5657 is a binary aluminum/magnesium alloy of moderate strength. It is not hardenable by heat treatment. It is strain hardenable. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-317. Producer or source: Various aluminum companies.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (8): Al-178.
Published: 01 August 1980
... ALUMINUM 5657 is an aluminum-base, wrought, non-heat-treatable alloy of high purity and bright appearance. It has high resistance to general corrosion and to stress-corrosion cracking. It is used widely in the anodized condition for automotive and appliance trim. This datasheet provides...
Abstract
View article
PDF
ALUMINUM 5657 is an aluminum-base, wrought, non-heat-treatable alloy of high purity and bright appearance. It has high resistance to general corrosion and to stress-corrosion cracking. It is used widely in the anodized condition for automotive and appliance trim. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-178. Producer or source: Various aluminum companies. Originally published August 1968, revised August 1980.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1988) 37 (6): SS-496.
Published: 01 June 1988
... Allegheny Ludlum AL 15-7 Alloy is a chromium-nickel-molybdenum-aluminum semi-austenitic stainless steel. It is heat treatable to high strength and it has a moderate level of corrosion resistance. It is available both as a conventionally melted product and as vacuum arc or electroslag refined...
Abstract
View article
PDF
Allegheny Ludlum AL 15-7 Alloy is a chromium-nickel-molybdenum-aluminum semi-austenitic stainless steel. It is heat treatable to high strength and it has a moderate level of corrosion resistance. It is available both as a conventionally melted product and as vacuum arc or electroslag refined material. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-496. Producer or source: Allegheny Ludlum Corporation.