Alloy Digest (1991) 40 (5): Al-316.
Published: 01 May 1991
... AA 5456 is a wrought aluminum-magnesium alloy of relatively high strength with good welding characteristics making it suitable for structural applications. (See also Aluminum 5456, Alloy Digest Al-70, September 1958.) This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1958) 7 (9): Al-70.
Published: 01 September 1958
... Aluminum 5456 is an aluminum-magnesium alloy suitable for structural welding applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on forming, heat...
Journal Articles
Alloy Digest (2013) 62 (1): Al-440.
Published: 01 January 2013
... are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum January 2013 Al-440 Endur-Al is an advanced 5456 alloy in H34...
Journal Articles
Alloy Digest (2002) 51 (6): Al-378.
Published: 01 June 2002
..., % Base alloy 317 46 165 24 22 As welded 310 45 159 23 14 Table 2 Typical Semiautomatic GMA Procedures for Fillet and LAP Welding Aluminum Wire DC (EP) range(a) DC (EP) suggested(a) Approximate diameter, in. Amps Volts Base thickness, in.(h) Amps Volts Wire feed, ipm Gas flow, cfh consumption, lb/100 ft(c...
Journal Articles
Alloy Digest (2003) 52 (1): Al-384.
Published: 01 January 2003
... Alcotec Weld filler wire 5183 is a non-heat-treatable aluminum welding wire whose principal alloying elements are magnesium, manganese, and chromium. It is similar to the European wire AlMg4.5Mn. This datasheet provides information on composition, physical properties, and tensile properties...
Journal Articles
Alloy Digest (1959) 8 (11): Al-85.
Published: 01 November 1959
.... 1477jNP5j6 Plate B.S. 1490,QMSM. castings u. s. Aluminum 5083 (approx.) Aluminum 5456 (approx.) General Characteristics: This alloy is eminently suitable for applications where a high standard of corrosion resistance is necessary with a good combination of rigidiy and high shock resistance. It requires...
Journal Articles
Alloy Digest (1988) 37 (7): Al-282.
Published: 01 July 1988
... Alcoa Aluminum Alloy 6013 is a high-strength Al-Mg-Si-Cu alloy. It is available in five tempers. It is crossing many market areas of applications in aerospace, defense, automotive and general structural use. This datasheet provides information on composition, physical properties, elasticity...