1-20 of 53 Search Results for

Aluminum alloys 2124

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (5): Al-413.
Published: 01 May 2008
... Kaiser aluminum alloy 2124 is a high-purity version of 2024 with tighter controls on the iron and silicon for an increase in strength and toughness. It is primarily used as plate in the aircraft industry. This data sheet applies to sheet, coil, and plate in the T851 temper. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (12): Al-310.
Published: 01 December 1990
... AA 2124 is a heat treatable aluminum plate alloy in which copper is the principal strengthening element. The alloy carries reduced allowable silicon and iron contents to ensure improved toughness. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2006) 55 (7): Al-399.
Published: 01 July 2006
...) temper, . ( circular-mil/ft) Mechanical Properties: Modulus of elasticity, GPa (106 psi) 73 (10.6) ALCOA 2124 PLATE Filing Code: Al-399 Aluminum July 2006 ALCOA 2124 PLATE (Aerospace Aluminum Alloy) Alloy 2124 is a heat treatable plate alloy that was developed for elevated-temperature application...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2008) 57 (7): Al-415.
Published: 01 July 2008
... Alcan 2297-T87 is an Al-Cu-Li-Mn-Zr alloy, developed to provide improved fatigue and damage tolerance with equivalent strength and corrosion resistance compared with incumbent alloy 2124-T851. The alloy possesses fatigue strength 3 to 5 times that of other aluminum alloys. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (9): SA-521.
Published: 01 September 2003
... Composition, wt (Typical) Carbon 0.10 Silicon 0.40 Manganese 1.5 Phosphorus 0.010 max Sulfur 0.01 max Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 276 356 (40 52) Yield strength after 2% strain and 414 (60...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (1): SA-528.
Published: 01 January 2004
... 0.20 Manganese 1.8 Phosphorus 0.02 max Sulfur 0.004 max Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 552 793 (80 115) Yield strength after 2% strain and 689 (100) baking 170 °C (340 °F) 20 mins, minimum...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (4): SA-534.
Published: 01 April 2004
... 0.015 max Sulfur 0.002 max Niobium 0.015 Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 496 752 (72 109) Yield strength, after 2% strain and 648 min (94 min) baking at 170 °C (340 °F) 20 min, MPa (ksi...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (10): SA-523.
Published: 01 October 2003
... toughness hardness heat treatability joinability mining industry physical properties tensile properties Chemical Composition, wt (Typical) Carbon 0.12 max Silicon 0.60 max Manganese 2.0 max Phosphorus 0.025 max Sulfur 0.010 max Aluminum 0.015 min Niobium 0.09 max Titanium 0.20 max Iron bal Physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (12): SA-542.
Published: 01 December 2004
... max Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 345 441 (50 64) Yield strength, after 2% strain and 496 min (72 min) baking at 170 °C (340 °F) 20 min, MPa (ksi) Tensile strength, MPa (ksi) 586-696 (85...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (8): SA-519.
Published: 01 August 2003
...) Carbon 0.13 Silicon 0.20 Manganese 1.5 Phosphorus 0.020 max Sulfur 0.004 max Niobium 0.015 Aluminum 0.04 Iron bal Physical Properties: Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 550 690 (80 100) Yield strength after 2% strain and 655 (95) baking 170 °C (340 °F...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (6): SA-537.
Published: 01 June 2004
... Silicon 0.20 Manganese 1.7 Phosphorus 0.02 max Sulfur 0.004 max Aluminum 0.04 Niobium 0.015 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 896 1138 (130 165) Yield strength, after 2% strain 1034 min (150 min) and baking...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (8): SA-539.
Published: 01 August 2004
... Silicon 0.20 Manganese 1.7 Phosphorus 0.020 max Sulfur 0.004 max Aluminum 0.04 Niobium 0.015 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 1034 1276 (150 185) Yield strength, after 2% strain and 1172 min (170 min) baking...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (9): Al-372.
Published: 01 September 2000
...). With relatively good fatigue resistance in plate forms, alloy 2024 continues in many aerospace structural applications. Chemical Composition, wt Silicon 0.50 max Iron 0.50 max Copper 3.8 4.9 Manganese 0.3 0.9 Chromium 0.10 max Zinc 0.25 max Titanium 0.15 max Others, each 0.05 max Others, total 0.15 max Aluminum...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (4): SA-616.
Published: 01 April 2010
.... DOCOL® 700W (Weather-Resistant Steel) DOCOL® 700W Chemical Composition, wt (Typical) Carbon 0.13 Silicon 0.5 Manganese 1.2 Phosphorus 0.01 Sulfur 0.002 Aluminum 0.04 Niobium 0.015 Chromium 0.5 Titanium 0.013 Copper 0.4 Iron bal Physical Constants: (Approximate) Density, kg/m3 (lb/in3) 7750 (0.280...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (2): SA-529.
Published: 01 February 2004
... 0.13 Silicon 0.20 Manganese 1.5 Phosphorus 0.015 max Sulfur 0.002 max Niobium 0.015 Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 496 648 (72 94) Yield strength, after 2% strain 648 min (94 min...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (3): SA-531.
Published: 01 March 2004
... 0.50 Manganese 1.5 Phosphorus 0.02 max Sulfur 0.004 max Niobium 0.015 Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 552 793 (80 115) Yield strength, after 2% strain 100 min (689 min) and baking at 170 °C...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (7): SA-538.
Published: 01 July 2004
... Composition, wt (Typical) Carbon 0.11 Silicon 0.20 Manganese 1.6 Phosphorus 0.015 max Sulfur 0.002 max Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 945 1207 (137 175) Yield strength, after 2% strain and 1124...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (1): SA-545.
Published: 01 January 2005
... products workability Chemical Composition, wt (Typical) Carbon 0.20 Silicon 0.20 Manganese 1.5 Phosphorus 0.025 max Sulfur 0.004 max Niobium 0.015 Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 7750 (0.280) Mechanical Properties: Yield strength, MPa (ksi) 1240 1480...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (2): SA-546.
Published: 01 February 2005
... joinability microstructure physical properties tensile properties transportation products wear resistance Chemical Composition, wt (Typical) Carbon 0.17 Silicon 0.50 Manganese 1.60 Phosphorus 0.01 max Sulfur 0.01 max Niobium 0.015 Aluminum 0.04 Iron bal Physical Properties: (Approximate) Density, kg...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (1): SA-613.
Published: 01 January 2010
... 0.02 Sulfur, max 0.003 0.003 Aluminum, min 0.015 0.015 Other Niobium Niobium Mechanical Properties: Mechanical properties and bending radius are shown in Table 1. Formability: Steel strip is the starting material for a whole range of different rails and profiles in vehicle manufacturing and other...