Alloy Digest (1965) 14 (9): Al-147.
Published: 01 September 1965
... Aluminum C612 is a natural aging aluminum permanent mold casting alloy that develops high mechanical properties without a quenching heat treatment. It has high shock resistance and excellent corrosion resistance. It is recommended for highly stressed castings. This datasheet provides information...