Alloy Digest (1963) 12 (9): Al-129.
Published: 01 September 1963
... Aluminum C113 is an aluminum permanent mold casting alloy having good pressure tightness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information...