Alloy Digest (1966) 15 (6): Al-156.
Published: 01 June 1966
... ALUMINUM B214 is an aluminum sand and permanent mold casting alloy recommended where excellent resistance to corrosion and tarnishing are required. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear strength. It also...
Journal Articles
Alloy Digest (1975) 24 (12): Al-220.
Published: 01 December 1975
... Equivalents: Sand Castings: AA No. B514.0 (Former Designation B214); ASTM B 26, B514.0 (GS42A); Federal QQ-A-60ld, B514.0 (B214 Ingots: AA No. B514.2 (Former designation B214); ASTM B 179, B514.2 (GS42A); Federal QQ-A-371e, B514.0 (B214). General Characteristics: Aluminum B5 14.0 is an aluminum-magnesium...
Journal Articles
Alloy Digest (1977) 26 (7): Al-227.
Published: 01 July 1977
...); Federal QQ-AdOld, B514.0 (B214). Ingots: AA No. B514.2 (Former designation B214); ASTM B 179, B5 14.2 (GS42A); Federal QQ-A-371e, B514.0 (B214). General Characteristics: Federated F024 is a sand-mold casting alloy containing nominally 2% silicon, 4% magnesium, and remainder aluminum. It is recommended...