Alloy Digest (1969) 18 (11): Al-192.
Published: 01 November 1969
... Aluminum A356 is a sand and permanent mold casting alloy that responds to an age-hardening heat treatment. It is recommended for aircraft and missile components where high strength and corrosion resistance are required. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1967) 16 (2): Al-163.
Published: 01 February 1967
... and very good solidification shrinkage tendency. It is similar to Aluminum A356 in all castable characteristics. This alloy produces pressure- tight castings. Weldability: This alloy is readily weldable by the oxyacetylene torch or gas shielded-arc process, using welding rod of the same composition...
Journal Articles
Alloy Digest (2020) 69 (12): Al-471.
Published: 01 December 2020
...-resistant alloys elasticity fatigue properties physical properties tensile properties ALCOA EVERCAST (C862F) (Al-4.8Zn-1.5Mg-0.68Cu-0.18V-0.18Zr Casting Alloy) Filing Code: Al-471 Aluminum :: December 2020 :: :: :: ::Materials Park, Ohio 44073-0002 440.338.5151 Fax 440.338.4634...
Journal Articles
Alloy Digest (1995) 44 (2): Al-332.
Published: 01 February 1995
... DURALCAN F3N.xxS is an aluminum composite with virtually no Cu or Ni designed for use in corrosion-sensitive applications. The matrix alloy is similar to 360 (See Alloy Digest Al-103, May 1961, and Al-245, April 1983). This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1992) 41 (7): Al-323.
Published: 01 July 1992
... Mold Castings) Alloys R-,4356.0, ER4010 and R4010 include aluminum-silicon-magnesium Almigweld and Altigweld filler wires with low iron content to weld alloys 356.0 and A356.0 (See Alloy Digest alloys Al-223 and 258). Composition*, Wt. %: Physical Properties: R-A356.0 R-A356.O/ER arid R4010 Element...
Journal Articles
Alloy Digest (2011) 60 (2): Al-435.
Published: 01 February 2011
... resistance as well as forming, machining, and joining. Filing Code: Al-435. Producer or source: Kaiser Aluminum. Producer or Source: Kaiser Aluminum Copyright © ASM International® 2011 2011 ASM International chemical composition corrosion-resistant alloys fatigue properties hardness...
Journal Articles
Alloy Digest (1994) 43 (10): Al-329.
Published: 01 October 1994
... Duralcan F3S.xxS is a heat treatable aluminum alloy-matrix gravity composite. The base alloy is similar to Aluminum 359 (Alloy Digest Al-188, July 1969); the discontinuously reinforced composite is silicon carbide. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2002) 51 (5): Al-377.
Published: 01 May 2002
... joinability physical properties tensile properties wrought aluminum alloys low-temperature alloys high-temperature alloys thermal properties UNS A95554 Chemical Composition, wt Silicon 0.25 max Iron 0.40 max Copper 0.10 max Manganese 0.05 1.0 Magnesium 2.4 3.0 Chromium 0.05 0.20 Zinc 0.25 max...
Journal Articles
Alloy Digest (1979) 28 (4): Al-234.
Published: 01 April 1979
... ALUMINUM A201 offers high strength, high impact resistance, a good combination of room and elevated-temperature performance, and good ballistic properties. Its ballistic properties are comparable to those of the standard wrought aluminum alloys. Among its many application are components...