Journal Articles
Alloy Digest (1952) 1 (3): Al-3.
Published: 01 November 1952
... Aluminum 61S is a wrought, heat-treatable alloy that combines the qualities of excellent resistance to corrosion, ease of fabrication and good mechanical properties. (See update, Aluminum 6061, Alloy Digest Al-205, January 1973.) This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1973) 22 (1): Al-205.
Published: 01 January 1973
... ALUMINUM 6061 is a wrought precipitation-hardenable aluminum alloy having excellent resistance to corrosion and good mechanical properties. (This alloy is covered under its old designation, ALUMINUM 61S, in Alloy Digest Al-3, November 1952.) This datasheet provides information on composition...
Journal Articles
Alloy Digest (2003) 52 (11): Ni-617.
Published: 01 November 2003
... This alloy improves upon the excellent high-temperature corrosion resistance of INCONEL alloy 690 (see Alloy Digest Ni-266, March 1981) through an addition of aluminum. Inconel Alloy 693 is typically 61% Ni, 29% Cr, 3.3% Al, and 0.7% Nb, with the balance being principally iron. By virtue of its...
Journal Articles
Alloy Digest (1958) 7 (1): Al-61.
Published: 01 January 1958
... castability chemical composition corrosion-resistant alloys dimensional stability ductility elasticity fatigue properties fracture toughness hardness heat treatability joinability machinability physical properties tensile properties APEX 417 Filing Cod.: Al-61 Aluminum AUoy % JANUARY 1958...
Journal Articles
Alloy Digest (1954) 3 (5): Al-16.
Published: 01 May 1954
... strength. It is produced in four tempers, namely, the annealed temper (0), the solution heat treated tempers (T3 & T4), and the solution heat treated and aged temper (T6). It has mechanical prop- erties comparable to alnminum alloy 14s and corro- sion resistance comparable to aluminum 61s. It is stable...
Journal Articles
Alloy Digest (1967) 16 (8): Ti-52.
Published: 01 August 1967
...& shows equiaxed alpha in an alpha plus kc* matrix. It is cwasidered to have signiRcant advantages for long time applications to 8WF. The bets stabilizing addition, molybdenum. increases room and elevated temperature tensile sttength nnd enhances rcrbilitv. The effect of the aluminum 61 the allo- tropic...
Journal Articles
Alloy Digest (1990) 39 (5): Cp-15.
Published: 01 May 1990
... resistance powder metal products SXA tensile properties - DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS SXA@ Filing Code: Composite cp15 MAY 1990 P&t&bed& Alby Digest hc.1201-677-6161 27 Canfii Slmet, Orange, NJ. 07650 I USA SXA= (Discontinuously Reinforced Aluminum Alloys) SXA@ is a unique group...
Journal Articles
Alloy Digest (2017) 66 (2): Al-453.
Published: 01 February 2017
... 0.15 max Aluminum bal Mechanical Properties: Table 1 and the data below present the statistically determined mechanical property minimums for Alclad 2029-T8 sheet and plate. The ultimate strength (Ftu) is similar to 2x24-T3/T351 products. However, Alclad 2029- T8 offers upwards of 20% improvement...
Journal Articles
Alloy Digest (1995) 44 (7): Al-337.
Published: 01 July 1995
... DURALCAN W2F.xxA is a heat-treatable wrought aluminum alloy matrix composite, where xx represents the volume percent of alumina particulate, Al2O3. The base alloy is aluminum 2618 (Alloy Digest Al-76, February 1959). This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1989) 38 (11): Al-232.
Published: 01 November 1989
..., physical properties, elasticity, tensile properties, and shear andbearing strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, and surface treatment. Filing Code: Al-232. Producer or source: Aluminum Company of America...
Journal Articles
Alloy Digest (2002) 51 (9): Ni-590.
Published: 01 September 2002
... Typical Carbon 0.05 0.15 0.08 Manganese 1.0 0.1 Silicon 0.5 0.1 Sulfur 0.015 0.002 Phosphorus 0.30 <0.01 Chromium 20.0 24.0 22 Nickel 50.0 bal 55 Niobium 1.0 <0.5 Iron 3.0 0.5 Copper 0.50 <0.2 Molybdenum 8.0 10.0 9 Cobalt 10.0 15.0 12 Aluminum 0.80 1.50 1 Titanium 0.60 0.3 Mechanical...
Journal Articles
Alloy Digest (1954) 3 (10): Al-21.
Published: 01 October 1954
... ALUMINUM 356 is a heat treatable aluminum casting alloy recommended for high strength, pressure-tight castings, and intricate shapes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (1990) 39 (1): Al-233.
Published: 01 January 1990
... ALCOA ALUMINUM ALLOY 7050 is an aluminum-zinc-copper-magnesium alloy with a superior combination of strength, stress-corrosion cracking resistance and toughness, particularly in thick sections. In thin sections it also possesses an excellent combination of properties that are important...
Journal Articles
Alloy Digest (1962) 11 (6): Al-115.
Published: 01 June 1962
... Aluminum C355 is a high purity permanent mold casting alloy that responds to an age-hardening heat treatment. It has superior properties to those of standard Aluminum 355. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1966) 15 (4): Al-154.
Published: 01 April 1966
... Aluminum 7039 is a wrought, heat treatable alloy having good weldability and good corrosion resistance combined with high strength. It is recommended for cryogenic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1987) 36 (3): SS-482.
Published: 01 March 1987
... INCOLOY ALLOY 800HT has improved creep and rupture strength due to closely controlled aluminum + titanium and carbon contents. In mill processing it receives a high-temperature grain-coarsening anneal which further contributes to high-temperature strength. This datasheet provides information...
Journal Articles
Alloy Digest (1985) 34 (1): Ni-308.
Published: 01 January 1985
... 0.25 max. Aluminum 1.5 max. Titanium 2.c3.5 Phosphorus 0.030 max. Others 0.50 max. PROPERTIES Table 1 - MINIMUM MECHANICAL PROPERTIES OF NICKEL FILLER METAL 61 (As-welded condition) Tensile strength, psi (M Pa) Yield strength (0.2% offset), psi (MPa) Elongation (4D), % 60000 (414) 35000 (241) 20...
Journal Articles
Alloy Digest (1954) 3 (7): Al-18.
Published: 01 July 1954
... ALUMINUM 355 is a heat treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for light weight, high strength, pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1954) 3 (1): Al-12.
Published: 01 January 1954
... BOHNALITE J is a high-copper aluminum alloy suitable for permanent mold and sand casting. It responds to heat treatment to produce high mechanical properties. It retains its strength well and has other excellent properties at elevated temperatures. Its bearing properties are also good...
Journal Articles
Alloy Digest (1954) 3 (9): Al-20.
Published: 01 September 1954
... ALCAN 135 is a heat treatable aluminum casting alloy having high strength, pressure tightness, and is capable of being cast in intricate shapes. It has high corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...