Journal Articles
Alloy Digest (1955) 4 (4): Al-25.
Published: 01 April 1955
... ALUMINUM 4032, formerly known as Aluminium 32S, is a forging alloy having comparatively low coefficient of expansion and good forgeability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well...
Journal Articles
Alloy Digest (1990) 39 (7): Al-305.
Published: 01 July 1990
...: Various aluminum companies Copyright © ASM International® 1996 1996 ASM International Aluminum alloys 4032 chemical composition coefficient of thermal expansion corrosion-resistant alloys fatigue properties forgeability hardness heat treatability high-temperature alloys joinability...
Journal Articles
Alloy Digest (1958) 7 (8): Al-68.
Published: 01 August 1958
... electrodes using direct current and reverse polarity (work negative). No flux is required in the inert-gas-shielded-~gsten-arc A. C. welding process. Specification Equivalents: British BS 1472 (or DTD 324A) Federal QQ-A-367 Cl. G Navy 4GA7 Cl. 6 SAE 290 AMS 4145 ASTM B247 Alloy SG 121A Aluminum 4032 General...
Journal Articles
Alloy Digest (1998) 47 (4): Al-347.
Published: 01 April 1998
...&338-4634 Mm-ServOpo.ASA.4~lntkq DELTALLOY 4032@ (Wear and Abrasion Resistant Alloy) Filing Code: Al-347 a Aluminum u - April 1998 Deltalloy 4032 has good machinability and drilling characteristics when using single-point or multispindle screw machines and an excellent surface finish using...
Journal Articles
Alloy Digest (2003) 52 (9): Ni-613.
Published: 01 September 2003
... thermal properties Chemical Composition, wt (Typical) Carbon 0.03 Chromium 25.0 Molybdenum 0.5 Cobalt 20.0 Aluminum 0.9 Titanium 1.8 Niobium 2.0 Manganese 0.30 Iron 0.7 Silicon 0.5 Nickel bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3 ) 8109 (0.293) Melting range, °C (°F) 1288 1362...