Journal Articles
Alloy Digest (1961) 10 (7): Al-105.
Published: 01 July 1961
... ALUMINUM 363 alloy is an aluminum-silicon-copper-zinc casting alloy having good tensile ductility in the as-cast condition. It responds to a solution and age-hardening treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1997) 46 (9): Be-9.
Published: 01 September 1997
... Beralcast 363, 191, and 310 are lightweight beryllium-aluminum (Be-Al) alloys for producing near net shapes by investment casting. Beralcast 363 is used primarily for structural applications, Beralcast 191 is used primarily for electronic packaging and Beralcast 310 for wrought products (from cast...
Journal Articles
Alloy Digest (1999) 48 (10): Al-363.
Published: 01 October 1999
... shown are typical, not to be used for specification or final design. Published by: ASM International Materials Park, Ohio 44073-0002 440-338-5151 Fax 440-338-4634 Mem-Serv@po.ASM-Intl.org FINKL ALU-X Filing Code: Al-363 Aluminum October 1999 Fig. 1 Temperature versus yield strength comparison between...
Journal Articles
Alloy Digest (1997) 46 (5): TS-555.
Published: 01 May 1997
.... mechanicaL and hydraulic forging presses. Imerts and tools have many applications in the production of steel, stainless. aluminum, magnesium forgings, and so forth. Note: An isothermal transformation diagram is available from the plWlllCeh. Products Available: DURODI is furnished in rings. disks. blocks...
Journal Articles
Alloy Digest (1988) 37 (10): Ni-363.
Published: 01 October 1988
... but is not generally used under such conditions unless other cormdents are involved. It is resistant o nonoxidizing salts. particularly halogens, such as aluminum chloride. Specification Equivalents: ASTM B333 ASME SB333 UNSN10665 General Characteristics: Resistance to pitting, sm -ioneraekingandintcrgranlllar aaack...
Journal Articles
Alloy Digest (2014) 63 (8): Ni-715.
Published: 01 August 2014
... Aluminum 4.0 Manganese 0.5 Silicon 1.5 Nickel bal Physical Properties: Density, kg/m3 (lb/in.3) 8290 (0.298) Melting range, °C (°F) 1357 1418 (2475 2585) Thermal coefficient of expansion, RT 1000 °C (RT 1832 °F), 10 6/K (10 6/°F) 17.2 (9.6) Thermal conductivity, W/m·K (Btu/(h·ft·°F)) 18.4 (10.6) Mechanical...
Journal Articles
Alloy Digest (1999) 48 (12): Al-364.
Published: 01 December 1999
... in- jection molds. For more demanding applications, Finkl s pre- mium forged aluminum product, Alu-X, is recommended (see Alloy Digest Al-363). Finkl Alu-C is 100% ultrasonically tested according to the most rigorous standards. It is fully warranted by the producer for molds. Product Forms Available: Aged...
Journal Articles
Alloy Digest (1988) 37 (12): Zn-45.
Published: 01 December 1988
... UNS Z33520 is a zinc-base alloy containing about 4% aluminum. It has no intentionally added copper. It is a relatively ductile (bendable and shapable) die casting alloy. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear...
Journal Articles
Alloy Digest (2006) 55 (3): SS-956.
Published: 01 March 2006
... 4 Copper 2.0 Titanium 0.9 Aluminum 0.4 Iron bal Density, kg/m3 (lb/in.3 ) 7900 (0.29) Resistivity at 20 °C (68 °F), . m 0.9 (540) ( circular-mil/ft) Thermal conductivity, aged condition, W/m . K (Btu/(ft . h . °F)) 20 °C (68 °F) 14 (7) 100 °C (200 °F) 16 (9) 200 °C (400 °F) 18 (10.5...
Journal Articles
Alloy Digest (2011) 60 (4): SA-623.
Published: 01 April 2011
... Heat Product Carbon <0.15 <.0.17 Silicon 0.10 0.50 0.05 0.56 Manganese 1.00 1.60 0.95 1.70 Phosphorus <0.020 0.025 Sulfur <0.003 <0.004 Nickel 0.60 1.00 0.55 10.05 Molybdenum 0.20 0.40 0.15 0.44 Chromium 0.20 0.40 0.15 0.45 Niobium <0.020 <0.025 Aluminum (total) >0.015 >0.015 Physical Properties...
Journal Articles
Alloy Digest (2005) 54 (7): Ni-626.
Published: 01 July 2005
... 0.5 max Chromium 16.0 20.0 Titanium 1.5 3.0 Aluminum 1.7 2.5 Cobalt 12.0 16.0 Molybdenum 5.0 9.0 Boron 0.005 max Zirconium 0.06 max Sulfur 0.015 max Nickel bal Physical Properties: Density, kg/m3 (lb/in.3 ) 8210 (0.297) Liquidus, °C (°F) 1345 (2453) Solidus, °C (°F) 1300 (2372) Specific heat capacity...
Journal Articles
Alloy Digest (2001) 50 (12): Ti-124.
Published: 01 December 2001
... ASM International bend strength chemical composition corrosion-resistant alloys creep properties elasticity fracture toughness high-temperature alloys physical properties RMI Ti BETA-C/Pd tensile properties thermal properties UNS R58645 Chemical Composition, wt Aluminum 3.0 4.0...
Journal Articles
Alloy Digest (2017) 66 (8): Ni-732.
Published: 01 August 2017
... Manganese 0.30 1.0 Chromium 20.0 24.0 Iron 3.0 max Molybdenum 1.0 3.0 Cobalt 3.0 max Tungsten 13.0 15.0 Lanthanum 0.01 0.05 Boron 0.015 max Aluminum 0.20 0.50 Nickel bal Physical Properties: Specific gravity 8.83 Density, kg/m3 (lb/in.3) 8830 (0.319) Electrical resistivity, RT, m ( circular-mil/ft) 1.25...
Journal Articles
Alloy Digest (1989) 38 (2): Zn-46.
Published: 01 February 1989
... UNS No. Z33531 is a zinc-base alloy containing about 4% aluminum and 1% copper. It is primarily a die casting alloy, having somewhat higher strength than UNS Z33521. This datasheet provides information on composition, physical properties, hardness, tensile properties, and compressive and shear...
Journal Articles
Alloy Digest (1991) 40 (9): SS-523.
Published: 01 September 1991
... stainless steel with excellent fracture toughness, transverse mechanical properties and stress-corrosion cracking resistance. It is produced by vacuum induction melting plus vacuum arc remelting. Composition (Typical Analysis): Carbon 0.04 Chromium 12.60 Nickel 8.30 Molybdenum 2.15 Aluminum 1.00 Iron Remain...
Journal Articles
Alloy Digest (1991) 40 (5): Ni-66.
Published: 01 May 1991
... NIMONIC ALLOY 105 is a wrought nickel-cobalt-chromium-base alloy strengthened by additions of molybdenum, aluminum and titanium. It has been developed for service up to 950 C (1742 F). This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also...
Journal Articles
Alloy Digest (2006) 55 (10): SS-977.
Published: 01 October 2006
... 13.50 16.00 Molybdenum 1.00 1.50 Vanadium 0.10 0.50 Boron 0.003 0.010 Aluminum 0.35 max Titanium 1.90 2.35 Nickel 24.00 27.00 Iron bal Physical Properties: Melting range, °C (°F) 1370 1425 (2500 2600) Density, kg/m3 (lb/in.3) 7910 (0.286) Magnetic permeability at H = 200 Oe Solution treated 1.006 Cold...
Journal Articles
Alloy Digest (2007) 56 (12): Ni-656.
Published: 01 December 2007
...) Carbon 0.06 Chromium 19.50 Iron 1.5 max Titanium 2.50 Aluminum 1.70 Nickel bal Physical Properties: Density, 20 °C (68 °F), kg/m3 (lb/in.3) 8200 (0.296) Thermal conductivity, 20 °C (68 °F), 13.0 (7.5) W/m · K (Btu/(ft · h · °F)) Specific heat capacity, 20 °C (68 °F), 460 (0.110) J/kg · K (Btu/lb · °F...
Journal Articles
Alloy Digest (1991) 40 (5): SA-37.
Published: 01 May 1991
..., balls, arbors. broach holders, rolls for aluminum rolling Producer: Carpenter Technology Corporation Carpenter &eel Division Reading, Pennsylvania 19612. 0 44 40 36 32 26 24 20 Fig. 2 - Core tensile properties vs hardness ...
Journal Articles
Alloy Digest (1967) 16 (5): TS-193.
Published: 01 May 1967
... suited for aluminum, zinc, and magnesium die casting dies. The vanadium increases its resistance to wash caused by the erosive actions of the molten die casting alloy, increases its resistance to heat checking, and imparts superior properties at elevated temperatures. This alloy also has excellent impact...