1-20 of 23 Search Results for

Aluminum 359

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1969) 18 (7): Al-188.
Published: 01 July 1969
... ALUMINUM 359 is a high strength, corrosion resistant aluminum casting alloy recommended for aircraft and missile applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength. It also includes...
Journal Articles
Alloy Digest (1994) 43 (10): Al-329.
Published: 01 October 1994
... Duralcan F3S.xxS is a heat treatable aluminum alloy-matrix gravity composite. The base alloy is similar to Aluminum 359 (Alloy Digest Al-188, July 1969); the discontinuously reinforced composite is silicon carbide. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1978) 27 (8): Cu-359.
Published: 01 August 1978
... equipment tensile properties wear resistance UNS C95500 Copper Alloy No. 955 Filing Code: cu-359 Copper Alloy AUGUST 1978 - DATA ON WORLD WIDE METALS AND ALLOYS w-&ff~m& h Upper Modchir, New Jersey Copper Alloy No. 955 (Heat-Treatable High-Strength Cast Aluminum Bronze) Copper Alloy No. 9.55 is a...
Journal Articles
Alloy Digest (1999) 48 (2): Al-359.
Published: 01 February 1999
... properties, tensile properties, and compressive, shear, and bearing strength as well as fatigue. It also includes information on as well as machining and surface treatment. Filing Code: AL-359. Producer or source: DWA Aluminum Composites. Producer or Source: DWA Aluminum Composites Copyright © ASM...
Journal Articles
Alloy Digest (1999) 48 (2): Al-358.
Published: 01 February 1999
... Kaiser Aluminum Alloy 2219 has good machinability and good mechanical properties. The alloy is typically used in high-temperature structural applications and is also used in high-strength weldments where postweld heat treatment can be employed. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1979) 28 (5): SA-359.
Published: 01 May 1979
... provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-359. Producer or source: Armco Inc., Eastern Steel...
Journal Articles
Alloy Digest (1976) 25 (6): Cu-313.
Published: 01 June 1976
... 359 and B 395. ASME: SB 111. SB 359 and SB 395. General Characteristics: Copper Alloy No. 687 is used widely for condenser tubes. It is very resistant to corrosion and erosion and has what is known as a self-healing skin. The addition of aluminum to copper alloy tubes makes them superior, in many...
Journal Articles
Alloy Digest (1982) 31 (8): Cu-443.
Published: 01 August 1982
... Copper Alloy No. C60800 is a medium-strength aluminum bronze containing nominally 95% copper and 5% aluminum. It has good resistance to atmospheric corrosion and its resists attack by nonoxidizing mineral acids such as sulfuric, hydrochloric and phosphoric. It is used widely for tubing in such...
Journal Articles
Alloy Digest (2005) 54 (4): Cu-733.
Published: 01 April 2005
... MoldStar 18 has good bearing qualities and has resistance to wear, abrasion, fatigue, deformation, and corrosion. MoldStar 21 and 22 are harder alloys and also have good bearing qualities and resistance to wear, abrasion, fatigue, deformation, and corrosion. This family of aluminum bronzes is used...
Journal Articles
Alloy Digest (1989) 38 (9): Al-299.
Published: 01 September 1989
... ALCOA Alloy 2090 is an aluminum-lithium alloy with 8% lower density and 12% higher elastic modulus than 7075-T6, a major high-strength alloy used in aircarft structures. Special facilities and practices required for casting commercial size aluminum-lithium ingots have been developed to cope with...
Journal Articles
Alloy Digest (2000) 49 (1): Cu-645.
Published: 01 January 2000
... Olin C688 is a brass enriched with both aluminum and cobalt for added strength and stress relaxation resistance. The alloy is ideal for springs. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. It also includes...
Journal Articles
Alloy Digest (2016) 65 (11): Al-448.
Published: 01 November 2016
... includes information on corrosion resistance as well as forming. Filing Code: Al-448. Producer or source: Kaiser Aluminum Corporation. Producer or Source: Kaiser Aluminum Corporation Copyright © ASM International® 2016 2016 ASM International chemical composition corrosion-resistant alloys...
Journal Articles
Alloy Digest (1998) 47 (5): Al-348.
Published: 01 May 1998
... Alcoa Excalibar 6013 alloy has high strength, good machinability, and good corrosion resistance. It is easily joined by all welding and brazing methods, has excellent compressive properties, and has good applied coating acceptance. See also Alcoa Aluminum Alloy 6013, Alloy Digest Al-282, revised...
Journal Articles
Alloy Digest (2008) 57 (1): Al-409.
Published: 01 January 2008
... max Iron 0.15 max Copper 3.9-4.9 Manganese 0.50-1.2 Magnesium 1.0-1.5 Zinc 0.20 max Titanium 0.08 max Zirconium 0.05-0.15 Aluminum bal Mechanical Properties: Mechanical properties and fatigue data are given in Table 1 and Fig. 1 and 2. Statistical A and B basis values, as well as a complete data...
Journal Articles
Alloy Digest (1984) 33 (9): Ni-302.
Published: 01 September 1984
... family of companies. Composition: Nickel 52.0 Chromium 22.0 Cobalt 12.5 Molybdenum 9.0 Aluminum I.2 Carbon 0.07 Iron 1.5 Manganese 0.5 Silicon 0.5 Sulfur 0.008 Titanium 0.3 Copper 0.2 Nominal for De- posited Filler Metal PROPERTIES Table 1 -TYPICAL OPERATING CONDITIONS FOR 0.045-in. (I.l-mm) DIAMETER...
Journal Articles
Alloy Digest (1991) 40 (8): Zn-51.
Published: 01 August 1991
... Copyright © ASM International® 1996 1996 ASM International cast zinc-aluminum alloys castability chemical composition compressive strength corrosion-resistant alloys elasticity fatigue properties fracture toughness hardness heat treatability joinability machinability physical properties...
Journal Articles
Alloy Digest (2004) 53 (4): Ni-620.
Published: 01 April 2004
... Aluminum 2.5 Iron bal Mechanical Properties: See Tables 1 and 2. Heat Treatment: The mechanical properties listed in Tables 1 and 2 are a result of the following heat treatment. Heat to 1168 °C (2135 °F) for 4 h and air cool, follow by heating to 1079 °C (1975 °F) for 4 h and air cooling, follow by heating...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-553.
Published: 01 July 1999
... Haynes International, Inc. Chemical Composition, wt (Nominal) Nickel Balance Chromium 16 Iron 8 Titanium 2.5 Niobium 1 Aluminum 0.8 Cobalt 1 max Manganese 0.35 max Silicon 0.35 max Carbon 0.08 max Physical Properties: Thermal conductivity, W/m K (Btu/(h · ft · °F)) 200 °C (392 °F) 14.1 (8.1) 400 °C (751...
Journal Articles
Alloy Digest (2011) 60 (1): Cu-794.
Published: 01 January 2011
... mechanical properties can be found in Table 1. Table 1 Mechanical properties Temper Tensile strength, MPa (ksi) Hardness HR 30-T (for information only) H00, 1 8 hard 221 276 (32 40) 49 max H02, ½ hard 255 317 (37 46) 43 57 H03, ¾ hard 283 345 (41 50) 47 59 H04, hard 296 359 (43 52) 54 62 H06, extra hard 324...
Journal Articles
Alloy Digest (1977) 26 (12): Ni-252.
Published: 01 December 1977
... Silicon 0.20 max. Specific heat, Btu/lb/oF (7@140oF) Phosphorus 0.015 max. kJ/kg.K (21-6OoC) 0.50 6.17 x 10-6 Sulfur 0.015 max. Thermal coef. expansion/OF (70-300oF) Chromium 22.7 (70-7000F) 7.92 x 10-6 Nickel Molybdenum Titanium Aluminum Columbium Boron iron 55.5 2.0 2.3 1.3 0.85 0.005 Remainder (70-l...