Skip Nav Destination
Close Modal
Search Results for
Aluminum 355
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 78 Search Results for
Aluminum 355
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1954) 3 (7): Al-18.
Published: 01 July 1954
... ALUMINUM 355 is a heat treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for light weight, high strength, pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Abstract
View article
PDF
ALUMINUM 355 is a heat treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for light weight, high strength, pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Al-18. Producer or source: Aluminum Company of America.
Journal Articles
Alloy Digest (1962) 11 (6): Al-115.
Published: 01 June 1962
... Aluminum C355 is a high purity permanent mold casting alloy that responds to an age-hardening heat treatment. It has superior properties to those of standard Aluminum 355. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Abstract
View article
PDF
Aluminum C355 is a high purity permanent mold casting alloy that responds to an age-hardening heat treatment. It has superior properties to those of standard Aluminum 355. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, machining, and joining. Filing Code: Al-115. Producer or source: Aluminum Company of America.
Journal Articles
Alloy Digest (1998) 47 (11): Al-355.
Published: 01 November 1998
.... It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: AL-355. Producer or source: Kaiser Aluminum Corporation. Producer or Source: Kaiser Aluminum Corporation Copyright © ASM International® 1998 1998 ASM...
Abstract
View article
PDF
Kaiser Aluminum alloy 2017 has good machinability and good mechanical properties. It is used in rivets. General structural applications, and transportation. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: AL-355. Producer or source: Kaiser Aluminum Corporation.
Journal Articles
Alloy Digest (1955) 4 (3): Al-24.
Published: 01 March 1955
... 4210; 4212 and 4214 Air Corps AN-A-40 Aluminum 355 British Standatd 1490-I-M-8 British DTD 716; 722; 727; 735 General Chamcteristics: BA.46 is one of the best casting alloys as it has ex- cellent casting qualities and retains its strength welI at elevated temperatures up to 400 deg. F. It is leak...
Abstract
View article
PDF
BA.46 is a heat treatable aluminum casting alloy. It is recommended for high strength, pressure-tight castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and machining. Filing Code: Al-24. Producer or source: The British Aluminium Company Ltd.
Journal Articles
Alloy Digest (1963) 12 (7): Al-127.
Published: 01 July 1963
..., kerosene, and kero- senclard oil mixrures are recommended for most machining operations. Castability: Good casting characteristics. The same partem equip- ment, Bating, risering, and melting practice may be used as for aluminum alloys 43. 108, 319, 355, and 3%. CASTINGTEMPERATURERANCE Sand 1250-1450oF...
Abstract
View article
PDF
LAVIN-CS 2700 is an aluminum casting alloy having a good combination of castability, machinability and corrosion resistance. It responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-127. Producer or source: R. Lavin & Sons Inc..
Journal Articles
Alloy Digest (1982) 31 (1): Al-235.
Published: 01 January 1982
...; AMS 4212; AMS 4214. Permanent-mold Castings: ASTM B 108, 355.0 (SCSIA); SAE 355.0 (322); Federal QQA-596, 355.0 (6); AMS 4280; AMS 4281. Ingots: The Aluminum 355.0 composition in ingot form is designated 355.1 (former designation 355). ASTM B 179,355-l (SCSlA and SCSlC); SAE 355.1 (322); Federal QQA...
Abstract
View article
PDF
ALUMINUM 355.0 is a general-purpose, high-strength casting alloy containing silicon and copper as the major alloying elements. Its casting characteristics are excellent and it is recommended for pressure-tight castings. It can be age hardened and has good resistance to corrosion. Among its uses are housings, cylinder heads and propeller gear boxes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-235. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1974) 23 (10): Al-209.
Published: 01 October 1974
... by standard corrosion tests. It has excellent resistance to most forms of corrosion; it is somewhat better than Aluminum 355 in this respect. Chemical conversion coatings give further protection. Specification Equivalents: Sand Castings: AA No. 356.0; ASTM B 26, 356.0 (SG70A); SAP 356.0 (323); Federal QQ...
Abstract
View article
PDF
Federated F070.3 is a heat-treatable aluminum casting alloy recommended for high strength, good corrosion resistance, pressue-tight castings and intricate shapes. It is normally used only when heat-treated (aged) strengths are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-209. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
Alloy Digest (1976) 25 (5): Al-223.
Published: 01 May 1976
... ALUMINUM 356.0 is an aluminum casting alloy that normally is used only when heat-treated (aged) strengths are required. It is recommended for high strength, pressure-tight castings, intricate shapes and good resistance to corrosion. Its many applications include gear cases, instrument housings...
Abstract
View article
PDF
ALUMINUM 356.0 is an aluminum casting alloy that normally is used only when heat-treated (aged) strengths are required. It is recommended for high strength, pressure-tight castings, intricate shapes and good resistance to corrosion. Its many applications include gear cases, instrument housings and components for aircraft and missiles. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-223. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (2014) 63 (12): SA-714.
Published: 01 December 2014
... Aluminum 0.02 Copper 0.40 Nickel 0.50 Molybdenum 0.10 Chromium 0.30 Vanadium 0.08 Niobium 0.05 Titanium 0.02 Nitrogen 0.010 Iron bal CEV = C+Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15; CET + C + (Mn+Mo)/10 + Cr + Cu)/20 + Ni/40 CEV and CET values based on plate thickness. See Table 1 for additional...
Abstract
View article
PDF
DI-MC 355 is a weldable fine-grained thermomechanically rolled steel for structural design. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-714. Producer or source: Dillinger Hütte GTS.
Journal Articles
Alloy Digest (1975) 24 (11): Al-219.
Published: 01 November 1975
... FEDERATED F150.5 is a heat-treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for high-strength, light-weight, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View article
PDF
FEDERATED F150.5 is a heat-treatable aluminum alloy containing silicon and copper as the major alloying elements. It is recommended for high-strength, light-weight, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as casting, heat treating, machining, and joining. Filing Code: Al-219. Producer or source: Federated Metals Corporation, ASARCO Inc..
Journal Articles
Alloy Digest (2015) 64 (9): SA-731.
Published: 01 September 2015
.... Chemical Composition, wt (Maximum) Carbon 0.12 Manganese 1.60 Silicon 0.50 Phosphorus 0.035 Sulfur 0.030 Aluminum 0.02 Chromium 0.30 Nickel 0.30 Molybdenum 0.20 Niobium 0.05 Titanium 0.05 Vanadium 0.10 Iron bal Upon agreement Si = 0.14 0.25% and phosphorus 0.035 maximum to form a zinc-rich layer during...
Abstract
View article
PDF
Histar 355 is a structural steel combining high yield strength (355 MPa minimum) with excellent toughness at low temperatures and outstanding weldability. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-731. Producer or source: ArcelorMittal and ArcelorMittal Luxembourg.
Journal Articles
Alloy Digest (2015) 64 (3): SA-721.
Published: 01 March 2015
... 0.50 1.25 Phosphorus 0.025 Sulfur 0.010 Aluminum 0.020 Copper 0.30 0.50 Nickel 0.50 Chromium 0.40 0.70 Niobium 0.015 0.05 Molybdenum 0.10 Zirconium 0.05 Iron bal CEV, % Plate thickness, 30 mm (1.2 in.) 0.46 Plate thickness, 60 mm (2.4 in.) 0.48 CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15...
Abstract
View article
PDF
Diweten 355 (minimum yield strength of 355 MPa, or 51 ksi, in thicknesses up to 16 mm, or 0.6 in.) is a structural steel with improved atmospheric corrosion resistance. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SA-721. Producer or source: Dillinger Hütte GTS.
Journal Articles
Alloy Digest (2015) 64 (12): SA-735.
Published: 01 December 2015
... 0.030 0.020 Sulfur 0.025 0.007 Aluminum 0.02 min 0.02 min Niobium 0.05 0.04 Titanium 0.025 0.025 Vanadium 0.06 0.06 Iron bal bal (a)Upon agreement: Si = 0.14 0.25% and P 0.035% max for capability to form a zinc rich layer during hot dip galvanizing. CEV max for OS is 0.39 and for TZK OS is 0.38...
Abstract
View article
PDF
Fritenar steels are structural steels combining high yield strength with excellent toughness at low temperatures and outstanding weldability. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on forming, machining, and joining. Filing Code: SA-735. Producer or source: ArcelorMittal.
Journal Articles
Alloy Digest (2008) 57 (10): SA-585.
Published: 01 October 2008
... 1.50 max Phosphorus 0.025 max Sulfur 0.010 max Aluminum 0.015 max Niobium 0.09(b) max Vanadium 0.20(b) max Titanium 0.15(b) max Iron bal (a) For hot dip galvanizing and thin zinc layer (50 80 m). (b) Sum of Nb, V, and Ti = 0.22 max Physical Constants: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280...
Abstract
View article
PDF
Domex 355 MC is a hot-rolled, high-strength low-alloy (HSLA) steel for cold forming operations. The alloy meets or exceeds the requirements of S355MC in EN 10149-2. This datasheet provides information on composition, physical properties, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: SA-585. Producer or source: SSAB Swedish Steel Inc.
Journal Articles
Alloy Digest (2016) 65 (5): SA-750.
Published: 01 May 2016
... 0.55 Aluminum, total 0.015 0.015 Niobium 0.05 0.09 Vanadium 0.20 Titanium 0.025 0.015 Iron bal bal CE, % = < 6 mm (0.24 in.) max = 0.17; > 6 mm (0.24 in.) = 0.29 CE = %C + %Mn/6 + (%Cu+%Ni)/15 + (%Cr + %Mo + %V)/5 Mechanical Properties: Mechanical properties are performed transverse to the rolling...
Abstract
View article
PDF
Ympress Laser S355MC (EN 10149-2) is a hot-rolled, high-strength, low-alloy steel with 355 MPa minimum yield strength. It is optimized for efficient laser cutting and post-cut processing. This datasheet provides information on composition, tensile properties, and bend strength as well as fracture toughness. It also includes information on forming. Filing Code: SA-750. Producer or source: Tata Steel.
Journal Articles
Alloy Digest (1995) 44 (8): Al-338.
Published: 01 August 1995
... ALUMINUM ALLOY 771.0 can be sand or permanent mold cast and naturally aged at room temperature. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, machining, joining, and surface...
Abstract
View article
PDF
ALUMINUM ALLOY 771.0 can be sand or permanent mold cast and naturally aged at room temperature. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting, heat treating, machining, joining, and surface treatment. Filing Code: AL-338. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1988) 37 (9): Al-291.
Published: 01 September 1988
...: Various aluminum companies. Producer or Source: Various aluminum companies Copyright © ASM International® 1996 1996 ASM International Aluminum alloys 355.0 cast aluminum-silicon alloys castability chemical composition corrosion-resistant alloys elasticity fracture toughness hardness...
Abstract
View article
PDF
AA 355.0 is a general-purpose, high-strength casting alloy containing silicon and copper as the major alloying elements. Its casting characteristics are excellent and it is recommended for pressure-tight castings. It can be age hardened and has good resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-291. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1968) 17 (5): Al-175.
Published: 01 May 1968
... Alloy 355 SAE 322 Aluminum Assoc. 355 General Characteri sties: Allcasr 41A is one of the best casting alloys as it has excellent foundv qualities and retains its strength well at elevated temperatures up to 40BF. It is leak-proof and pressure right. It also responds well co the age- hardening heat...
Abstract
View article
PDF
ALLCAST 41A is an aluminum-silicon-copper casting alloy. It responds to an age-hardening heat treatment and is recommended for light weight, high strength, pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance as well as heat treating, machining, and joining. Filing Code: Al-175. Producer or source: Apex Smelting Company.
Journal Articles
Alloy Digest (1996) 45 (8): Ni-515.
Published: 01 August 1996
.... Chemical Composition, wt (Deposited Weld Metal) Carbon MW== Iron Phosphorus Sulfur Aluminum Copper SiIiCOll Titauilml ClWOtilUll Molybdenum Tungsten Nickel 0.02 max. 1.0 max. 5.0 max. 0.02 max. 0.02 max. . . . 0.5 max. 0.25 max. 0.25 max. 19.0-23-o 15.0-17.0 3.0-4.4 0.5 max. Balance General Characteristics...
Abstract
View article
PDF
Inco-Weld Welding Electrode 686CPT is an all-position shielded-metal-arc (SMAW) electrode with highter (CR + Mo + W) content than most other nickel-base welding products. This higher alloy content increases the resistance to pitting, crevice, and general corrosion. Applications include the severest service in pollution control engineering. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-515. Producer or source: Inco Alloys International Inc.
Journal Articles
Alloy Digest (2009) 58 (7): Al-423.
Published: 01 July 2009
... Aluminum has long been accepted as a mold material. This alloy has a combination of faster machining, highest heat transfer, lighter weight, higher strength in thick sections, and greater thermal conductivity than other aluminum alloys. This datasheet provides information on physical properties...
Abstract
View article
PDF
Aluminum has long been accepted as a mold material. This alloy has a combination of faster machining, highest heat transfer, lighter weight, higher strength in thick sections, and greater thermal conductivity than other aluminum alloys. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties. It also includes information on forming and machining. Filing Code: AL-423. Producer or source: Alcoa Forged and Cast Products.