Skip Nav Destination
Close Modal
Search Results for
Aluminum 354.0
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-2 of 2 Search Results for
Aluminum 354.0
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (7): Al-204.
Published: 01 July 1972
... ALUMINUM 354.0 is a permanent-mold casting alloy that responds to an age-hardening heat treatment. It has good strength, weldability and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep and fatigue...
Abstract
View article
PDF
ALUMINUM 354.0 is a permanent-mold casting alloy that responds to an age-hardening heat treatment. It has good strength, weldability and corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as heat treating, machining, and joining. Filing Code: Al-204. Producer or source: Aluminum Company of America.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2021) 70 (8): Al-479.
Published: 01 August 2021
... Rio Tinto 354.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting to be used for the production of sand and permanent mold castings. Alloy 354.0 was developed especially for premium engineered casting...
Abstract
View article
PDF
Rio Tinto 354.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting to be used for the production of sand and permanent mold castings. Alloy 354.0 was developed especially for premium engineered casting applications requiring high strength and elongation, and sound castings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting and heat treating. Filing Code: Al-479. Producer or source: Rio Tinto Limited.