1-20 of 21 Search Results for

Aluminum 319

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1964) 13 (10): Al-140.
Published: 01 October 1964
... Aluminum 319 is a general purpose foundry alloy moderately responsive to heat treatment. It has excellent casting characteristics and good mechanical properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive...
Journal Articles
Alloy Digest (1991) 40 (9): Al-319.
Published: 01 September 1991
... AA 6351 wrought alloy contains silicon and magnesium in such amounts that Mg2Si is present as the precipitation hardening constituent with proper heat treatment. The 6000 series alloys are less strong than most of the 2000 and 7000 series aluminum alloys. The formability and corrosion resistance...
Journal Articles
Alloy Digest (1963) 12 (7): Al-127.
Published: 01 July 1963
...-Relief Anneal: Hear at 4SO-475oF for 2-4 hours, depending on section site, and air cool. Machinability: CS 2700 has rhe same good machinability as Aluminum 108 and Aluminum 319. In the as-cast condition, before aging, castings will be gummy and difficult to machine like Aluminum 43 would be. The same...
Journal Articles
Alloy Digest (1962) 11 (6): Al-8.
Published: 01 June 1962
... cast in this alloy than in the alloys of high copper content. ALLCAST 60 is similar to Aluminum Alloy 319 as marketed by other aluminum alloy manufacturers. Forms Available: Ingots, sand castings and permanent mold castings. Applications: Ornamental castings, highly stressed castings, pressure tight...
Journal Articles
Alloy Digest (1983) 32 (10): Cu-464.
Published: 01 October 1983
... applications include bearings, bushings, pump impellers and corrosion-resistant castings. Composition: Nominal Range Copper* Tm Lead Nickel Zinc Antimony Iron Sulfur Phosphorus l * Aluminum Silicon 78 75.cb79.0 7 6.3-7.5 I5 13.sl6.0 - 1.0 max. - 0.8 max. - 0.8 max. - 0. I5 max. - 0.08 max. - 0.05 max. - 0.005...
Journal Articles
Alloy Digest (1956) 5 (12): Al-46.
Published: 01 December 1956
... strength as well as fatigue. It also includes information on heat treating, machining, and joining. Filing Code: Al-46. Producer or source: Bohn Aluminum & Brass Corporation. Producer or Source: Bohn Aluminum & Brass Corporation Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (2004) 53 (10): SS-911.
Published: 01 October 2004
... 0.025 max Chromium 13.5 16.0 Nickel 24.0 27.0 Molybdenum 1.0 1.5 Titanium 1.90 2.35 Aluminum 0.35 max Boron 0.003 0.010 Vanadium 0.10 0.50 Iron bal Physical Properties: Melting range, °C (°F) 1371 1427 (2500 2600) Density, kg/m3 (lb/in.3 ) 7940 (0.287) See also Fig. 1. Mechanical Properties: Hardness...
Journal Articles
Alloy Digest (1998) 47 (5): Al-348.
Published: 01 May 1998
... Alcoa Excalibar 6013 alloy has high strength, good machinability, and good corrosion resistance. It is easily joined by all welding and brazing methods, has excellent compressive properties, and has good applied coating acceptance. See also Alcoa Aluminum Alloy 6013, Alloy Digest Al-282, revised...
Journal Articles
Alloy Digest (1985) 34 (12): Fe-71.
Published: 01 December 1985
.... Composition: Chromium Aluminum Iron Nominal Composition: 22.0 5.25 Remainder Physical Constants: Density, g/cu cm Melting point, C (Approximate) Specific heat, J/g/ C Thermal coef. expansion/ C (20-250°C) (20-500°C) (20-750°C) (20-looo c) Thermal conductivity. W/m / C (At 20°C) Electrical resistivity. ohm...
Journal Articles
Alloy Digest (1985) 34 (5): Al-256.
Published: 01 May 1985
... ALUMINUM 319.0 is a general-purpose foundry alloy that is moderately responsive to heat treatment. It has excellent casting characteristics and good mechanical properties. Among its many uses are crankcases, housings, engine parts, typewriter frames and rear-axle housings. This datasheet provides...
Journal Articles
Alloy Digest (1996) 45 (6): Cu-605.
Published: 01 June 1996
... is a registered trademark. Chemical Composition(a), wt Copper 86.0-88.0 Tin 4.0-6.0 Lead 0.25 Zinc 4.0-6.0 Bismuth 0.5-1.5(b) Selenium 0.35-0.7(b) Nickel (including cobalt) 1.0 Iron 0.30 Antimony 0.25 SIllflU 0.08 Phosphorus 0.05 Aluminum 0.005 Silicon 0.005 Sum of named elements 99.3 min. (a) max. unless range...
Journal Articles
Alloy Digest (2011) 60 (9): SS-1101.
Published: 01 September 2011
... resistance at high temperatures. CRONIFER® 40B (High Temperature Alloy) CRONIFER® 40B Chemical Composition, wt Chromium 2.0 23.0 Carbon 0.012 Manganese 1 Silicon 1.3 2.2 Copper 0.5 Phosphorus 0.03 Nitrogen 0.35 0.6 Aluminum 0.5 Lanthanum 0.03 0.20 Sulfur 0.03 Nickel 36.0 39.0 Iron bal Physical Properties...
Journal Articles
Alloy Digest (2006) 55 (3): SS-956.
Published: 01 March 2006
... 4 Copper 2.0 Titanium 0.9 Aluminum 0.4 Iron bal Density, kg/m3 (lb/in.3 ) 7900 (0.29) Resistivity at 20 °C (68 °F), . m 0.9 (540) ( circular-mil/ft) Thermal conductivity, aged condition, W/m . K (Btu/(ft . h . °F)) 20 °C (68 °F) 14 (7) 100 °C (200 °F) 16 (9) 200 °C (400 °F) 18 (10.5...
Journal Articles
Alloy Digest (2014) 63 (5): Ti-154.
Published: 01 May 2014
... deep hardening forging alloy. TIMETAL® GRADE 17 (High Strength Forging Alloy) TIMETAL® GRADE 17 Chemical Composition, wt Min Max Nominal Aluminum 4.5 5.5 5.0 Tin 1.6 2.4 2.0 Zirconium 1.6 2.4 2.0 Chromium 3.5 4.5 4.0 Molybdenum 0.4 max 0.3 Nickel 0.9 max 0.8 Iron 0.30 max 0.15 Oxygen 0.2 max 0.16...
Journal Articles
Alloy Digest (1958) 7 (12): Ni-48.
Published: 01 December 1958
...-bearing gases above 700 F. (371 C Molten sulfur auacks Mod 403 at temperatures over 500°F. (260°C Molten metals, such as lead, tin, zinc, and aluminum, corrode at high raa. Pickling: Heat-formed oxides are resistant m acid pickling baths. Corn- mercially these are reduced before pickling by heating...
Journal Articles
Alloy Digest (1998) 47 (8): Cu-621.
Published: 01 August 1998
...-lnn.ofg OLIN 172 (High Beryllium Copper) 01~ I72 has a relatively hrgh beryllium content and the ability to reach tensile strengths near 1380 MPa (200 ksi) Chemical Composition, wt Beryllium Nickel + cobalt Nickel + cobalt + roe Aluminum Silicon Copper 1.8~LXt0 0.20 min 0.6 max 0.20 max 0.20 max BalanCe...
Journal Articles
Alloy Digest (1980) 29 (10): SA-377.
Published: 01 October 1980
... requiring high-strength steels. Any load- carrying component can be considered a possible candidate for an INX Steel. Toughness: Toughness is Influenced greatly by steelmaking practice, roll- ing practice, section thickness and strength level. In general, if good toughness is a requirement, aluminum-killed...
Journal Articles
Alloy Digest (2000) 49 (11): Cb-25.
Published: 01 November 2000
... Aluminum <20 Magnesium <20 Molybdenum <20 Lead <20 Cobalt <10 Boron <1 Physical Properties: Density, kg/m3 (lb/in.3 ) 8850 (0.320) Coefficient of linear thermal expansion, 10 6/K (10 6/°F)(a) 95 °C (200 °F) 6.8 (3.8) 980 °C (1800 °F) 7.7 (4.3) 1095 °C (2000 °F) 7.9 (4.4) 1205 °C (2200 °F) 8.1 (4.5) Thermal...
Journal Articles
Alloy Digest (2022) 71 (10): CS-233.
Published: 01 October 2022
... with liquid brass, aluminum bronze, copper, zinc, Table 2 Physical properties Property Liquidus temperature Density Coefficient of linear thermal expansion Thermal conductivity Specific heat capacity Electrical resistivity Unit °C (°F) kg/m3 (lb/in.3) 10 6/K (10 6/°F) W/(m K) (Btu/(h·ft·°F)) J/(kg K) (cal/(g...
Journal Articles
Alloy Digest (2022) 71 (2): CS-216.
Published: 01 February 2022
..., aluminum bronze, copper, zinc, lead-tin solders, lithium, cadmium and indium. The degree of embrittlement is greater for steels that have been heat treated to produce higher strength. Source: Ref 22 Corrosion in Fresh Water. The average corrosion rate of nonalloy steels in stagnant air-saturated soft...