Alloy Digest (1969) 18 (3): Al-185.
Published: 01 March 1969
... ALUMINUM 2014 is a heat treatable alloy having high tensile and fatigue strength. It is recommended for fittings, hardware, aircraft engine components, structures, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear...
Journal Articles
Alloy Digest (1998) 47 (10): Al-354.
Published: 01 October 1998
... Kaiser Aluminum alloy 2014 is one of the strongest heat-treatable alloys for screw machine applications. The alloy has good machinability and high strength. Corrosion resistance is only fair. Weldability is good with arc and resistance methods. In many applications, this alloy can be substituted...
Journal Articles
Alloy Digest (1990) 39 (5): Al-304.
Published: 01 May 1990
... AA 2014 is a precipitation hardenable aluminum alloy in which copper is the principal alloying element. In the heat treated condition the alloy's properties are similar to those of mild steel. Corrosion resistance of AA 2014 is inferior to that of most other aluminum alloys. Sheet and plate may...
Journal Articles
Alloy Digest (1995) 44 (5): Al-334.
Published: 01 May 1995
... DURALCAN W2A.xxA-T6 is a heat-treatable wrought aluminum alloy metal-matrix composite, where xx represents the volume percent of alumina particulate, Al2O3. The base alloy is 2014 (Alloy Digest Al-185, March 1969). This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (2020) 69 (11): Al-470.
Published: 01 November 2020
...) (a) Source: Properties and Selection of Aluminum Alloys, Volume 2B, ASM Handbook, ASM International, 2019, p 353 Mechanical Properties Atlas 5052 is not hardenable by heat treatment. Like all the 5xxx series aluminum alloys, it can be significantly strength- ened by cold working, enabling a series of H...
Journal Articles
Alloy Digest (2014) 63 (8): Ni-715.
Published: 01 August 2014
... Aluminum 4.0 Manganese 0.5 Silicon 1.5 Nickel bal Physical Properties: Density, kg/m3 (lb/in.3) 8290 (0.298) Melting range, °C (°F) 1357 1418 (2475 2585) Thermal coefficient of expansion, RT 1000 °C (RT 1832 °F), 10 6/K (10 6/°F) 17.2 (9.6) Thermal conductivity, W/m·K (Btu/(h·ft·°F)) 18.4 (10.6) Mechanical...
Journal Articles
Alloy Digest (2014) 63 (4): Al-441.
Published: 01 April 2014
... International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440-338-8542 www.asminternational.org Filing Code: Aluminum April 2014 Al-441 Alcoa has developed this special grade of alloy 5182 for construction of road tankers. ALCOA ALLOY 5182 RTSG1 (High-Strength...
Journal Articles
Alloy Digest (2014) 63 (3): SA-694.
Published: 01 March 2014
... 1000 LCE Chemical Composition, wt (Typical) Carbon 0.12 Silicon 0.40 Manganese 2.80 Phosphorus 0.020 Aluminum 0.015 min Sulfur 0.010 Niobium + titanium 0.10 max Iron bal CE = C + Mn/20 + Si/30 + 2P + 4S 0.25 Physical Constants: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280) Mechanical Properties...
Journal Articles
Alloy Digest (2014) 63 (2): Ti-151.
Published: 01 February 2014
... is an + alloy with excellent creep resistance and high strength. TIMETAL® 7-4 (Alpha-Beta Titanium Alloy) TIMETAL® 7-4 Chemical Composition, wt Min Max Nominal Aluminum 6.50 7.30 6.90 Molybdenum 3.50 4.50 4.00 Iron 0.15 0.30 0.20 Oxygen 0.16 0.20 0.18 Carbon 0.010 Nitrogen 0.05 Hydrogen 0.013 Residual elements...
Journal Articles
Alloy Digest (2014) 63 (5): SA-701.
Published: 01 May 2014
... Chemical Composition, wt (Typical) Carbon 0.12 Silicon 0.40 Manganese 2.80 Phosphorus 0.020 Aluminum 0.015 min Sulfur 0.010 Niobium + Titanium 0.10 max Iron bal CE = C + Mn/20 + Si/30 + 2P + 4S = 0.25 Physical Constants: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280) Mechanical Properties: Yield...
Journal Articles
Alloy Digest (2014) 63 (12): SA-715.
Published: 01 December 2014
... Steel) DOCOL® 1000 DPZE Chemical Composition, wt (Typical) Carbon 0.18 Silicon 0.80 Manganese 1.80 Phosphorus 0.020 Aluminum 0.015 min Sulfur 0.010 Niobium + Titanium 0.10 max Iron bal Physical Properties: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280) Mechanical Properties: Yield strength, min...
Journal Articles
Alloy Digest (2014) 63 (1): SA-689.
Published: 01 January 2014
... chemical composition. The ZE suffix in the title signifies that is electrogalvanized. DOCOL® 1400 MZE (Electrogalvanized Ultra High-Strength Steel) DOCOL® 1400 MZE Chemical Composition, wt (Typical, maximum) Carbon 0.20 Silicon 0.4 Manganese 1.6 Phosphorus 0.020 Sulfur 0.01 Aluminum, total 0.015 min...
Journal Articles
Alloy Digest (2014) 63 (3): Ti-152.
Published: 01 March 2014
... alloy with excellent creep resistance. TIMETAL® 8-1-1 (Alpha-Beta Titanium Alloy) TIMETAL® 8-1-1 Chemical Composition, wt Min Max Nominal Aluminum 7.35 8.3 7.85 Vanadium 0.75 1.25 1.0 Molybdenum 0.75 1.25 1.0 Iron 0.15 Oxygen 0.06 0.12 0.85 Carbon 0.08 Nitrogen 0.05 Hydrogen 0.004 Residual elements...
Journal Articles
Alloy Digest (2021) 70 (1): Ti-174.
Published: 01 January 2021
...) Ti6Al4V(a) Element (c) (d) (e) Nitrogen 0.01 Carbon 0.0.03 0.05 0.05 0.05 (a) For wrought Ti-6Al-4V alloy. Source: ATI. (b) At 0 316 °C (32 600 °F) Hydrogen 0.003 Iron 0.10 0.08 0.10 0.08 Table 2 Mechanical properties at room Oxygen 0.15 temperature Aluminum 0.015 0.015 0.015(e) Vanadium 6 Yttrium 4 0.30...
Journal Articles
Alloy Digest (2014) 63 (11): SS-1189.
Published: 01 November 2014
... 1.00 1.00 Manganese 2.00 2.00 Phosphorus 0.040 0.025 Sulfur 0.030 0.025 Nickel 24.00 27.00 24.00 27.00 Chromium 13.50 16.50 13.50 16.00 Molybdenum 1.00 1.50 1.00 1.50 Aluminum 0.35 0.35 Titanium 1.90 2.35 1.90 2.35 Boron 0.001 0.020 0.003 0.010 Vanadium 0.10 0.50 0.10 0.50 Iron bal bal Cobalt 1.00...
Journal Articles
Alloy Digest (2014) 63 (12): SA-714.
Published: 01 December 2014
... Aluminum 0.02 Copper 0.40 Nickel 0.50 Molybdenum 0.10 Chromium 0.30 Vanadium 0.08 Niobium 0.05 Titanium 0.02 Nitrogen 0.010 Iron bal CEV = C+Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15; CET + C + (Mn+Mo)/10 + Cr + Cu)/20 + Ni/40 CEV and CET values based on plate thickness. See Table 1 for additional...
Journal Articles
Alloy Digest (2002) 51 (11): Al-382.
Published: 01 November 2002
... International aircraft structural components ALCOTEC WELD FILLER WIRE 2319 chemical composition joinability physical properties tensile properties wires wrought aluminum alloys thermal properties UNS A92319 Chemical Composition, wt Silicon 0.20 max Iron 0.30 max Copper 5.8 6.8 Manganese 0.20...
Journal Articles
Alloy Digest (2014) 63 (3): SA-696.
Published: 01 March 2014
... as nitrides by means of aluminum and, where applicable, niobium or titanium. Mechanical Properties: Hardness at room temperature In annealed condition 300 HBW In quenched and tempered condition > 550 HBW Delivery Condition. Annealed, quenched, or quenched and tempered (see the section, Heat Treatment...
Journal Articles
Alloy Digest (2014) 63 (4): Ni-666.
Published: 01 April 2014
.... INCOLOY® ALLOY 945 AND 945X (Sour Gas Service Nickel Alloy) INCOLOY® ALLOY 945 AND 945X Chemical Composition, wt (Nominal) Nickel 45.0 55.0 Chromium 19.5 23.0 Molybdenum 3.0 4.0 Niobium 2.5 4.5 Copper 1.5 3.0 Titanium 0.5 2.5 Aluminum 0.01 0.7 Manganese 1.0 max Silicon 0.5 max Sulfur 0.03 max Phosphorous...
Journal Articles
Alloy Digest (2014) 63 (2): SA-693.
Published: 01 February 2014
...) Carbon 0.20 Manganese 1.50 Phosphorus 0.020 Sulfur 0.010 Silicon 0.60 Chromium 0.60 Molybdenum 0.50 Nickel 1.00 Niobium 0.040 Vanadium 0.070 Titanium 0.040 Aluminum 0.070 Nitrogen 0.014 Boron 0.005 Iron bal CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Ni+Cu)/15, typical 0.40 CET= C + (Mn+Mo)/10 + Ni/40 + (Cr+Cu)/20...