Alloy Digest (1955) 4 (12): Al-35.
Published: 01 December 1955
... ALUMINUM 142 is a heat treatable aluminum casting alloy recommended for services at elevated temperatures. It has high strength and good wear resistance in the fully heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1964) 13 (1): TS-142.
Published: 01 January 1964
... CROMO-N tool steel is a low-carbon, high-chromium grade, specially developed to provide optimum resistance to heat-checking during service at elevated temperatures. It is recommended for aluminum die casting dies, extrusion press tooling, aluminum and copper forging dies, and mandrels...
Journal Articles
Alloy Digest (1964) 13 (12): Al-142.
Published: 01 December 1964
..., tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-142. Producer or source: Aluminum Company of Canada Ltd. Producer...
Journal Articles
Alloy Digest (1957) 6 (12): Al-60.
Published: 01 December 1957
... watet.It is subject to intercrystalline attack. Specification Equivalents: ASTM B247 Al. CN42D ASTM B179 Al. CN42D ASTM B108 Alloy CN42D ASTM B26 Alloy CN42D AMS 4220 and 4222 Federal QQ-A-601 Comp. G Federal QQ-A-596 Comp. 3 Federal QQ-A-371 Comp. F MIL-A-958 Cl. 3 AN-A-32 SAE 39 Aluminum 142 General...
Journal Articles
Alloy Digest (1971) 20 (5): Al-202.
Published: 01 May 1971
... Characteristics: ALUMINUM 242.0, formedy called Aluminum 142 or Y alloy, is a casting alloy containing copper, nickel, and magnesium. It can be heat treated to improve the mechanical properties and stabilize the dimensions against undesirable changes during operation at elevated temperatures. It also has good...
Journal Articles
Alloy Digest (1974) 23 (12): Al-212.
Published: 01 December 1974
... FEDERATED F401.5Ni is a heat-treatable aluminum casting alloy with high strength and good wear resistance in the fully heat-treated condition. It is recommended for castings requiring good strength at elevated temperatures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2001) 50 (9): Ti-119.
Published: 01 September 2001
... strength chemical composition creep properties elasticity forgings fracture toughness high-temperature alloys joinability physical properties sheets tensile properties titanium-aluminum-tin-zirconium-molybdenum-silicon alloys thermal properties Ti-6Al-2Sn-2Zr-2Mo-0.15Si alloy is used...
Journal Articles
Alloy Digest (2018) 67 (1): Al-456.
Published: 01 January 2018
... and heat treating. Filing Code: Al-456. Producer or source: Kaiser Aluminum Corporation. Producer or Source: Kaiser Aluminum Corporation Copyright © ASM International® 2018 2018 ASM International chemical composition corrosion-resistant alloys elasticity fatigue properties hardness heat...
Journal Articles
Alloy Digest (2007) 56 (10): Ti-142.
Published: 01 October 2007
... creep resistance elasticity fracture toughness heat treatability joinability physical properties shear strength tensile properties Timetal 685 workability thermal properties Chemical Composition, wt Aluminum 5.70-6.30 Zirconium 4.50-6.00 Molybdenum 0.25-0.75 Silicon 0.015-0.35 Iron 0.05 max...
Journal Articles
Alloy Digest (1954) 3 (2): Al-13.
Published: 01 February 1954
... CERALUMIN C is an age-hardenable aluminum alloy having good high temperature properties with exceptional fatigue strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on high...
Journal Articles
Alloy Digest (2023) 72 (7): Ni-784.
Published: 01 July 2023
... Böhler L090 is a wrought, precipitation-hardenable, nickel-chromium-cobalt alloy that is strengthened by additions of titanium and aluminum. It has been developed as an age-hardenable creep resisting alloy for service at temperatures up to 900 °C (1650 °F). This datasheet provides information...
Journal Articles
Alloy Digest (1963) 12 (4): SS-142.
Published: 01 April 1963
... nitric acids, nitric-sulphuric mixtures, acetic, citric and lactic acids. Resistance to Corrosion Character of Salt by Molten Salts Drawing % tempering fair Neutral fair Cyaniding fair High speed fair Resistance to Corrosion Metal by Molten Metals Lead !vd Aluminum not resistant hlagn esium not resistant...
Journal Articles
Alloy Digest (1990) 39 (1): Fe-89.
Published: 01 January 1990
... 0.015 max. Chromium 0.50 max. Nickel 38.00 cobalt 14.00 Titanium 1.60 Columbium + tantalum 4.90 Aluminum 0.15 max. Copper 0.50 max. Boron 0.012 max. Iron Remainder Physical Constants: Density, lb/cu in. Specific gravity Thermal coef. expansion/ F (77-200°F) (77-400°F) (77~600°F) (77-800°F) (77-1000°F...
Journal Articles
Alloy Digest (2021) 70 (7): Al-478.
Published: 01 July 2021
... 156 136 142 (ksi) (22 23) (20 21) General Characteristics % 17 23 14.7 17.3 Non-heat-treatable; suitable for high pressure die castings; (a) To compare with a conventional AlSi10MnMg alloy, test samples were cut from a casting characteristics are not as good as those of aluminum- specified location...
Journal Articles
Alloy Digest (1991) 40 (8): Cer-6.
Published: 01 August 1991
... and wear resistance. Dies and rollers used in aluminum steel forming, pump shafts and bearings. Producers: Kyocera Industrial Ceramics Corp. Vancouver. Cl ashington 98661. DOI: 10.31399/asm.ad.cer0006 Copyright © ASM International® 1996 ...
Journal Articles
Alloy Digest (1955) 4 (8): Al-30.
Published: 01 August 1955
... ALUMINUM 5357 is an aluminum-magnesium-manganese alloy of the non-heat-treatable type. Formerly known as Aluminum C57S or Aluminum K157. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear and bearing strength. It also includes...
Journal Articles
Alloy Digest (2008) 57 (6): Al-414.
Published: 01 June 2008
... Kaiser Aluminum alloy 7175/7475 is a high-purity version of 7075 and is heavily used by the aircraft and ordinance industries because of its superior strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2014) 63 (3): SA-694.
Published: 01 March 2014
... 1000 LCE Chemical Composition, wt (Typical) Carbon 0.12 Silicon 0.40 Manganese 2.80 Phosphorus 0.020 Aluminum 0.015 min Sulfur 0.010 Niobium + titanium 0.10 max Iron bal CE = C + Mn/20 + Si/30 + 2P + 4S 0.25 Physical Constants: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280) Mechanical Properties...
Journal Articles
Alloy Digest (1963) 12 (3): SA-142.
Published: 01 March 1963
... -3200F co9OOoF. It is a marrensitic steel strengthened by precipitation and an ordering reaction. Composition: Carbon 0.03 max. Silicon 0.10 max. Manganese 0.10 max. SUlfUI 0.03 max. Phosphorus 0.03 max. Molybdenum 4.60-5.00 Nickel 18.00-19.00 Cobalt 7.00-8.50 Titanium .30-.50 Aluminum .05-.15 Boron .006...
Journal Articles
Alloy Digest (2014) 63 (5): SA-701.
Published: 01 May 2014
... Chemical Composition, wt (Typical) Carbon 0.12 Silicon 0.40 Manganese 2.80 Phosphorus 0.020 Aluminum 0.015 min Sulfur 0.010 Niobium + Titanium 0.10 max Iron bal CE = C + Mn/20 + Si/30 + 2P + 4S = 0.25 Physical Constants: (Approximate) Density, kg/m3 (lb/in.3) 7750 (0.280) Mechanical Properties: Yield...