Alloy Digest (1958) 7 (11): Al-72.
Published: 01 November 1958
... ALUMINUM 13 is a die casting alloy having excellent castability and good corrosion resistance. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature...
Journal Articles
Alloy Digest (1965) 14 (10): Cu-156.
Published: 01 October 1965
... Wearite 4-13 is a corrosion and wear resistant extruded aluminum bronze preheat treated to high strength and hardness levels. It is recommended for sliding contact applications where wear resistance and non-galling characteristics are desired. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1955) 4 (12): CI-13.
Published: 01 December 1955
... NITRICASTIRON is a chromium, aluminum, molybdenum iron having a surface capable of being hardened to a high degree in an atmosphere of ammonia at temperatures below 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1962) 11 (1): Cu-13.
Published: 01 January 1962
... BRIDGEPORT 712 is a highly corrosion resistant aluminum-silicon bronze having good spring characteristics. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat...
Journal Articles
Alloy Digest (1954) 3 (2): Al-13.
Published: 01 February 1954
... fatigue properties hardness heat treatability high-temperature alloys joinability machinability physical properties tensile properties mng cod.: AI-13 CERALUMIN C Aluminum Alloy FEBRUARY, 1954 - DATA ON WORLD WIDE METALS AND AUOYS CERALUMIN C (Nidd-Aluminum High Strong%, Low Weight Casting...
Journal Articles
Alloy Digest (1992) 41 (3): SS-525.
Published: 01 March 1992
... ALFA I and ALFA II ALLOYS are 13% chromium ferritic stainless steels with 3 and 4% aluminum, respectively. These steels have superior oxidation resistance. Being ferritic they are not hardenable by heat treatment. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1953) 2 (10): Al-9.
Published: 01 October 1953
... method. The die casting characteristics, how- ever, are slightly inferior to those of Ahlmixlum 13 or 380 aIloys and quaI to those of Aluminum 85 alloy. However, casting shapes of great intricacy is illlptaceicaL Corrosion Resistance: Exceknt resistance to corrosion and to discoloration. For added...
Journal Articles
Alloy Digest (1967) 16 (8): Al-168.
Published: 01 August 1967
...-168 Aluminum Allov I nLurrBInurrrn 13 I , AUGUST 1967 -DATA ON WORLD WIDE METALS AND ALLOYS ALUMINUM-Al3 Pmbiirbed by Engineering Alloys Digest, Inc. Upper Montclair. NW Jerss (Die Casting Alloy) Aluminum-Al3 is a high-silicon. aluminum-base alloy recommended for applications where excellent...
Journal Articles
Alloy Digest (1957) 6 (8): Al-54.
Published: 01 August 1957
... Aluminum 13 or 39 alloys. In the as-cast condition it has a high? strength, a greater endurance limit, better machmmg charac- teristics, and is more ductile than Aluminum 13 die- casting alloy. The fatigue properties are comparable to values attained with wrought aluminum alloys. The alloy has a lower...
Journal Articles
Alloy Digest (1965) 14 (5): Al-145.
Published: 01 May 1965
... pressure tightness, and excellent die filling capacity. General Characteristics: Aluminum 364 combines high strength formerly found only in Aluminum 218 (which can be cast only in simple shapes) and the excellent casting properties of Aluminum 13. It has alloying elements to improve mechanical properties...
Journal Articles
Alloy Digest (1977) 26 (12): Al-231.
Published: 01 December 1977
... ALUMINUM 413.0 is normally classified as a die-casting alloy; however, it also can be used for sand and permanent-mold castings. Its high silicon content (12%) lowers its melting temperature and increases its fluidity, thus improving its castability. It is used for intricate thin-walled castings...
Journal Articles
Alloy Digest (1998) 47 (12): Al-356.
Published: 01 December 1998
.... No straightening takes place after stretching. Specification Equivalents: UNSA92111 Producer: Temulum Jackson, TN 38301 (800) USE-20 11 (901) 427-6499 (fax) Temulum is a Division of Kaiser Aluminum Corporation Houston, TX 77257-2887 (7 13) 267-3777 (7 13) 267-3741 (fax) ISSN: 002-614X DOI: 10.31399/asm.ad.al0356 ...
Journal Articles
Alloy Digest (1990) 39 (1): Al-233.
Published: 01 January 1990
... ALCOA ALUMINUM ALLOY 7050 is an aluminum-zinc-copper-magnesium alloy with a superior combination of strength, stress-corrosion cracking resistance and toughness, particularly in thick sections. In thin sections it also possesses an excellent combination of properties that are important...
Journal Articles
Alloy Digest (2011) 60 (3): Al-436.
Published: 01 March 2011
... information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming and joining. Filing Code: Al-436. Producer or source: Kaiser Aluminum. See also Alloy Digest Al-458, July...
Journal Articles
Alloy Digest (1992) 41 (3): Al-322.
Published: 01 March 1992
... AA 5052 is a non heat treatable aluminum/magnesium alloy of moderate strength and good weldability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on corrosion...
Journal Articles
Alloy Digest (1976) 25 (2): Al-221.
Published: 01 February 1976
... FEDERATED F0120 is a high-silicon aluminum alloy suitable for sand, permanent-mold and die casting. It is used for intricate thin-walled castings requiring pressure tightness, toughness and good resistance to corrosion. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1966) 15 (4): Al-154.
Published: 01 April 1966
... Aluminum 7039 is a wrought, heat treatable alloy having good weldability and good corrosion resistance combined with high strength. It is recommended for cryogenic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1979) 28 (6): Al-131.
Published: 01 June 1979
... ALUMINUM 6053 is a wrought aluminum alloy that can be hardened and strengthened by aging. It is characterized by moderate strength, good formability and excellent resistance to corrosion. This alloy is used widely for rivets. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2008) 57 (6): Al-414.
Published: 01 June 2008
... Kaiser Aluminum alloy 7175/7475 is a high-purity version of 7075 and is heavily used by the aircraft and ordinance industries because of its superior strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1990) 39 (5): Al-304.
Published: 01 May 1990
... AA 2014 is a precipitation hardenable aluminum alloy in which copper is the principal alloying element. In the heat treated condition the alloy's properties are similar to those of mild steel. Corrosion resistance of AA 2014 is inferior to that of most other aluminum alloys. Sheet and plate may...