Alloy Digest (1957) 6 (2): Al-48.
Published: 01 February 1957
... ALUMINUM 122 is an aluminum sand and permanent mold casting alloy recommended for applications where good high temperature strength, high hardness, resistance to wear and good machinability are required. It responds to an age-hardening heat treatment. This datasheet provides information...
Journal Articles
Alloy Digest (1962) 11 (11): Cu-122.
Published: 01 November 1962
... joinability machinability physical properties tensile properties Tuf-Stuf 224E-75 workability All Or DIQXST Filing Code: Cu-122 TUF-STUF 224E-75 copper Alloy NOVEMBER 1962 -DATA ON WORLD WIDE METALS AND ALLOYS TUF-STUF 224E-75 (Aluminum Bronze) Publisbd by Engineering Alloys Digest, Inc. upper...
Journal Articles
Alloy Digest (1963) 12 (2): Al-122.
Published: 01 February 1963
... castability chemical composition corrosion-resistant alloys elasticity fatigue properties fracture toughness hardness machinability physical properties shear strength tensile properties APEX Z39-11 Filing Code: AI-122 Aluminum Alloy FEBRUARY 1963 -DATA ON WORLD WIDE METALS AND ALLOYS Published...
Journal Articles
Alloy Digest (1974) 23 (11): Al-211.
Published: 01 November 1974
... of Aluminum 222.0 was Aluminum 122. Sand Castings: ASTM B 26, 222.0 (CGlOOA); SAE 222.0 (34): Federal QQ-AdOld, 222.0 (122). Permanent-Mold Castings: ASTM B 108, 222.0 (CGIOOA); SAE 222.0 (34); Federal QQA-596d. 222.0 (2). Ingots: ASTM B 179.222.1 (CGlOOA); SAE 222.1 (34); Federal QQ-A-371e, 222.1 (122...
Journal Articles
Alloy Digest (1954) 3 (1): Al-12.
Published: 01 January 1954
... Corporarion, Detroit, Michigan Also produced as Aluminum 122 aIloy by: Aluminum Company of America, Pittsburgh. Pmnspivania Reynolds Metals Company, Louisville. Kenrucky Kaiser Alum.inllm % chemical co., Oakland California 1 Or DIGEST CARPENTER No. -876 RltgcokfA-8 -w DECRMEER 19E2 DATA ON WORLD WIDE METALS...
Journal Articles
Alloy Digest (2012) 61 (9): SA-662.
Published: 01 September 2012
... that combine high strength with excellent forming and welding performance. RQT 501 (Q & T Structural Steel) RQT 501 Chemical Composition, wt (Typical analysis, for 8 t 100) Carbon 0.20 Manganese 1.60 Phosphorus 0.025 Silicon 0.60 Sulfur 0.010 Molybdenum 0.60 Vanadium 0.10 Nickel 1.00 Aluminum...
Journal Articles
Alloy Digest (1955) 4 (11): Al-34.
Published: 01 November 1955
... HIDUMINIUM RR.58 is a heat treatable aluminum alloy recommended for high temperature applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high...
Journal Articles
Alloy Digest (1968) 17 (7): Al-177.
Published: 01 July 1968
...: Most of the ocher aluminum casting alloys race above this alloy in resistance co corrosion, but its resistance co corrosion is entirely suitable for many applications. Specification Equivalents: ASTM Alloy CG 1OOA QQ-A-371 Alloy G QQ-A-596 Cl. 2 QQ-A-601 Alloy 122 SAE 34 AA 122 General Characteristics...
Journal Articles
Alloy Digest (1989) 38 (8): Al-298.
Published: 01 August 1989
... FVS 0812 is a rapidly solidified Al-Fe-V Sialloy which combines the strength, ductility and fracture toughness of conventional aerospace aluminum alloys with the high-temperature strength and stability of the FVS aluminum alloys. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2001) 50 (9): Ti-119.
Published: 01 September 2001
... strength chemical composition creep properties elasticity forgings fracture toughness high-temperature alloys joinability physical properties sheets tensile properties titanium-aluminum-tin-zirconium-molybdenum-silicon alloys thermal properties Ti-6Al-2Sn-2Zr-2Mo-0.15Si alloy is used...
Journal Articles
Alloy Digest (1973) 22 (8): Al-208.
Published: 01 August 1973
... VANASIL 77 is an age-hardenable hypereutectic aluminum-silicon casting alloy having a low coefficient of thermal expansion and excellent wear resistance. These factors, combined with excellent high-temperature strength make it an excellent material for applications where light weight is required...
Journal Articles
Alloy Digest (2012) 61 (1): Al-438.
Published: 01 January 2012
... Al-SiC is a 68% volume fraction alpha-silicon carbide aluminum alloy. Al-SiC materials provide superior thermal management for high technology electronics applications in a lightweight, cost-effective material. This datasheet provides information on composition, physical properties, microstructure...
Journal Articles
Alloy Digest (2001) 50 (2): SA-508.
Published: 01 February 2001
... Phosphorus 0.020 max Sulfur 0.010 max Silicon 0.15 0.45 Chromium 2.2 2.6 Molybdenum 0.90 1.10 Titanium 0.05 0.10 Vanadium 0.20 0.30 Boron 0.0015 0.0070 Nitrogen 0.012 max Aluminum 0.020 max Iron bal Physical Properties: Density, kg/m3 (lb/in.3) 7840 (0.283) Thermal conductivity, W/m · K (Btu/(ft · h · °F...
Journal Articles
Alloy Digest (2001) 50 (1): SA-507.
Published: 01 January 2001
... operating parameters of pressure and temperature. Chemical Composition, wt Carbon 0.04 0.10 Manganese 0.10 0.60 Phosphorus 0.030 max Sulfur 0.010 max Silicon 0.50 max Chromium 1.9 2.6 Molybdenum 0.05 0.30 Vanadium 0.20 0.30 Tungsten 1.45 1.75 Niobium 0.02 0.08 Boron 0.0005 0.0060 Nitrogen 0.030 max Aluminum...
Journal Articles
Alloy Digest (2016) 65 (12): Cu-854.
Published: 01 December 2016
.... Filing Code: Cu-854. Producer or source: Kobe Steel Ltd, Aluminum and Copper Business. Producer or Source: Kobe Steel Ltd, Aluminum and Copper Business Copyright © ASM International® 2016 2016 ASM International bend strength chemical composition electronic applications hardness KOBELCO...
Journal Articles
Alloy Digest (1961) 10 (11): SA-122.
Published: 01 November 1961
... quenching, by the action of partially dissociated ammonia gas at temperatures from about 925-1025oF. l Nitralloy - Trademark of The Nirralloy Corp. Composition: Physical Constants: Carbon 0.25-0.35 Manganese 0.40-0.60 Silicon 0.30 max. Aluminum 1.00-l .50 Molybdenum 0.60-l .OO Iron Remain,ler Density, lb...
Journal Articles
Alloy Digest (1990) 39 (9): Al-307.
Published: 01 September 1990
... AA 6066, like other 6XXX aluminum series alloys, contains magnesium and silicon in approximate proportions to form Mg2Si, the constituent responsible for the precipitation hardening capability of the alloy. AA6066 develops intermediate strength levels when heat treated and it possesses good...
Journal Articles
Alloy Digest (1990) 39 (12): Al-310.
Published: 01 December 1990
... AA 2124 is a heat treatable aluminum plate alloy in which copper is the principal strengthening element. The alloy carries reduced allowable silicon and iron contents to ensure improved toughness. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1972) 21 (12): Ni-182.
Published: 01 December 1972
... environments. The properties make it attractive for applications in aerospae and process industries as welI as automotive thermal reactor core components. *ALTEMP is a registered trademark of ABegheny Ludlum Industries, Inc. Composition: Typical Nickel chrOllliUlll Iron Aluminum Carbon Manganese Sulfur Silicon...
Journal Articles
Alloy Digest (1964) 13 (12): Al-142.
Published: 01 December 1964
... Aluminum AI32 ASTM Alloy SN 122A SAE 321 BS 1490-LM-13 CSA Alloy SN 122 General Characteristics: Alcan 162 is a high silicon-aluminum alloy recom- mended for pistons and other applications where high strength, ductility, corrosion resistance and pressure tighmess are required. It is an age- hardenable...