Alloy Digest (1969) 18 (10): Fe-40.
Published: 01 October 1969
... Alnico-IV is an un-oriented permanent-magnet iron-base alloy. It is a general purpose alloy for use where space limitations make short magnets necessary. It is supplied in the as-cast or as-sintered condition. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1969) 18 (12): Cu-209.
Published: 01 December 1969
...\ . 01 . a\ 1 .-SINTERED ALNICO II 2.-SINTERED ALNICO IV 3.-SINTERED 4.-SINTERED 5.-VECTOUTE 6.dUNIFE I I x DE&WhETU.NG FORCE-H - OEM TEDS c-rCLI L Demagnetization and energy product curves for sintered magnetic materials. Heat Treatment: General Characteristics: Heat at 1900oF for 4 hours. quench in oil...