Alloy Digest (1968) 17 (7): Fe-34.
Published: 01 July 1968
... ALNICO-I is an un-oriented permanent magnet iron-base aloy recommended for general purposes in electrical and magnetic equipment. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining...
Journal Articles
Alloy Digest (1967) 16 (11): Fe-31.
Published: 01 November 1967
... ALNICO II is a general purpose permanent magnet alloy recommended for applications where better magnetic properties than Alnico I are desired. It is a high coercive force, high energy magnetic alloy. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1968) 17 (6): Fe-33.
Published: 01 June 1968
... properties ALNICO-I I I Filing Code: Fe-33 Iron Alloy JUNE 1968 - DATA ON WORLD WIDE METALS AND ALLOYS Plrblisbed by Engineering Alloys Digest, Inc. Upper Montclair, New Jersey ALNICO-III (Permanent Magnet) t\LNICO III is a general purpose iron-nickel-aluminum permanent magnet alloy. It is hard...
Journal Articles
Alloy Digest (1966) 15 (10): Fe-29.
Published: 01 October 1966
... 7000000 Table 3 - TYPICAL MECHANICAL PROPERTIES Tensile strength, psi 5000 Transverse modulus of rupture, psi 8000 Rockwell hardness c50 DEMAGNETIZATION CURVE ENERGY PRODUCT AND B/H VALUES ALNICO 5-7 r 6 x H I: IO- 7.0 6.0 5.0 LO 3.0 LO I.0 I 14.0 3.0 2.0 1 .o 0.0 9.0 6.0 ; 7.0 2 1 60; 5.0 00 3.0 2.0 I...
Journal Articles
Alloy Digest (1962) 11 (4): Fe-20.
Published: 01 April 1962
... Hyflux Alnico V-7 is a high energy permanent magnet capable of achieving typical energy values of 7 million BH max. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code...
Journal Articles
Alloy Digest (1969) 18 (10): Fe-40.
Published: 01 October 1969
... 3000 3100 3100 Sintered TEMPERATURE (DEGREES F 1 Napneric rernxence vs. temperatures for various grades of Xlnico. DOI: 10.31399/asm.ad.fe0040 Copyright © ASM International® 1996 i- DEMAGNETIZATION CURVES +ENE;~RDucT~ - 6 ALNICO 6 - I2 ALNICOIZ _ -H 1000 800 600 400 200 0 I 2 3 4 5x106 Heat Treatment...
Journal Articles
Alloy Digest (1964) 13 (8): Co-39.
Published: 01 August 1964
... Alnico 8 is a permanent magnet material having over twice as much resistance to demagnetization as Alnico 5. It requires a magnetic heat treatment to develop strong directional magnetic properties. This datasheet provides information on composition, physical properties, and hardness. It also...
Journal Articles
Alloy Digest (1963) 12 (9): Fe-17.
Published: 01 September 1963
... ALNICO V is an oriented permanent magnet alloy. It has the highest energy product of all material. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: Fe-17. Producer...
Journal Articles
Alloy Digest (1963) 12 (4): Fe-23.
Published: 01 April 1963
... approximately 11/32 of an inch to the foot when cast. General Characteri rtics: ALNICUS is cast modified Alnico V-DG permanent magnet alloy improved by directional solidification. The high energy product (BH max.) of Alnicus exceeds dear of the available Alnico alloys. OaIy platinum-cobalt alloys show...
Journal Articles
Alloy Digest (1981) 30 (6): Co-77.
Published: 01 June 1981
.... (For magnets operabig at [Bd Hd] maximum point) REVERSIBLE TEMPERATURE FFECTS Flux change et various temperatures Varrations in flux output due to nversibfe characteristics at various temperatures are shown in this chart for Alnico, fndox and tncor. (For magnets operating at fld Hd] maximum point) I Fig. 1...
Journal Articles
Alloy Digest (1981) 30 (8): Co-78.
Published: 01 August 1981
... - DATA ON WORLD WIDE METALS AND ALLOYS @I Copyri9ht 1980. En9imering Publications, Inc. Ail rights reserved. IssN:002614x INCOR* 18 and 21 (Rara-Earth Cobalt Magnet Materials) INCUR 18 and 21 are new permenent magnet materials; they are dosely related to Incor 16 (Alloy Digest, Co-77, June 1981). Incor...
Journal Articles
Alloy Digest (1969) 18 (12): Cu-209.
Published: 01 December 1969
...\ . 01 . a\ 1 .-SINTERED ALNICO II 2.-SINTERED ALNICO IV 3.-SINTERED 4.-SINTERED 5.-VECTOUTE 6.dUNIFE I I x DE&WhETU.NG FORCE-H - OEM TEDS c-rCLI L Demagnetization and energy product curves for sintered magnetic materials. Heat Treatment: General Characteristics: Heat at 1900oF for 4 hours. quench in oil...
Journal Articles
Alloy Digest (1956) 5 (6): SA-44.
Published: 01 June 1956
... composition cobalt magnet steel coercive force elasticity heat treatability machinability physical properties workability I OPI COBALT MAGNET STEEL Filing Code: SA-44 Steel Alloy JUNE 1956 DIGESTa - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbd by Engineering Alloys Digest, Inc Upper Montchxir, New...
Journal Articles
Alloy Digest (1988) 37 (10): Fe-86.
Published: 01 October 1988
... (Parallel to M) (Perpendicular to M) Electrical resistivity. microhm-cm (At 25°C) *Dependent on operating slope and duty cycle. Magnetic Characteristics: Peak energy density, B,H,, MGG WI@ Residual induction Br, Gauss mT Coercive force Hc, Gersted Intrinsic coercive force Hci, Gersted Magnetizing force I...
Journal Articles
Alloy Digest (1961) 10 (8): Cu-105.
Published: 01 August 1961
... CUNIFE-I is a permanent magnet alloy recommended where magnets must be formed or machined, as this material is ductile, malleable and machinable after heat treatment. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...