1-6 of 6 Search Results for

Almar 25

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1963) 12 (9): SA-154.
Published: 01 September 1963
... ALMAR 25 is a maraging alloy steel having an excellent combination of strength and toughness particularly in the presence of notches or cracks. It is recommended for applications such as fuel rocket cases and aircraft landing gears. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1967) 16 (4): SA-208.
Published: 01 April 1967
... ALMAR 362 is a maraging stainless steel having high corrosion and oxidation resistance. It has good workability and weldability with low rate of work hardening. It is recommended for chemical processing and industrial equipment industries requiring high strength material with outstanding corrosion...
Journal Articles
Alloy Digest (1970) 19 (2): SS-234.
Published: 01 February 1970
... ALLEGHENY ALMAR-362 is an age-hardenable martensitic stainless steel recommended for applications requiring high strength and good corrosion resistance, such as aircraft and missile structures, hydraulic and pneumatic equipment components, and in the chemical processing industry. This datasheet...
Journal Articles
Alloy Digest (1963) 12 (10): SA-156.
Published: 01 October 1963
... ALMAR 18 is a high-nickel martensitic steel which is strengthened by precipitation hardening. It has excellent combination of strength and toughness particularly in the presence of notches or cracks. It is recommended for applications such as solid fuel rocket cases and aircraft landing gears...
Journal Articles
Alloy Digest (1964) 13 (4): SA-162.
Published: 01 April 1964
... ALMAR 20 is a high nickel martensitic steel which is strengthened by precipitation hardening. It has excellent combination of strength and toughness particularly in the presence of notches and cracks. It is recommended for applications such as solid fuel rocket cases and aircraft landing gear...
Journal Articles
Alloy Digest (1974) 23 (7): SS-297.
Published: 01 July 1974
... hour. Machinability: Allegheny Stainless AM-363 has moderately good machinability, as shown in the following tabulation: Relative Machinability for AlJoy Constant Tool Life AlSl Type 304 100% Almar*- 111% AM-363 150% AISI Type 416 310% Test condition: Tool - /4 inch M-l drill, Gulf cutting oil 43A...