Alloy Digest (1991) 40 (2): Ni-392.
Published: 01 February 1991
... ALLVAC RENE 41 in the age-hardened condition has exceptionally high strength at room temperature and in the 1200-1800 F (649-982 C) temperature range. It is produced by double vacuum melting (induction + vacuum arc or induction + electroslag remelting). This datasheet provides information on...
Journal Articles
Alloy Digest (1964) 13 (4): Ni-90.
Published: 01 April 1964
... limitation-and for such other alloy will be preferred as a Rene 41 alloy. Corrosion Resistance: This alloy has a high resistance to rosion. It also has a high resistance and scaling at elevated temperatures. Pickling: joints some filler, e.g., general car to oxidation For removal of hot work oxide the part...