Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... HASTELLOY Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2019) 68 (5): Ni-752.
Published: 01 May 2019
... Hastelloy C-22 welding wire is used on Hastelloy alloy C-22, an excellent corrosion resistant material with exceptional diversity. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: Ni-752. Producer...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (7): Ni-437.
Published: 01 July 1993
... Alloy C-22 is a nickel-chromium-molybdenum alloy that has outstanding resistance to pitting, crevice corrosion and stress-corrosion cracking. The alloy also has excellent resistance to both reducing and oxidizing media. The alloy has good mechanical properties at both room and elevated...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2017) 66 (10): Ni-737.
Published: 01 October 2017
... Sandvik Sanicro 59 is a corrosion resistant grade (CRA) available as wire, particularly weld wire. Sanicro 59 is used to weld most of the nickel alloys such as alloy 59, C-22, C-276, etc. It can also be used for joining nickel alloys with duplex stainless steels, super duplex stainless steels...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (11): SS-660.
Published: 01 November 1996
... CLI-50A is a Korean 6 Mo superaustenitic stainless steel with improved corrosion resistance properties. The chromium additions have been increased up to 22% together with high nitrogen additions. The PREN value [%Cr] + 3.3 [%Mo] + 16[%N] is higher than 45. The alloy is copper free. This alloy...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (6): SS-506.
Published: 01 June 1989
... heat, Btu/lbPF(120-210 F) 0.015 (480-570°F) 0.005 JlkgPC (50- 100°C) 25 (250-300°C) 22 Thermal coef. expansionPF x 10 (70-210 F) 2.2 (70-390 F) 0.12 (70-570 F) Remainder PC x lo6 (20-100°C) (20-200°C) (20-300°C) Thermal conductivity. Btu/ft*/ft/hr/ F (70°F) (At 210°F) (At 57O F) W/m C (At 20°C...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2012) 61 (5): SS-1121.
Published: 01 May 2012
... Crofer 22 H is an improved high performance material for use in high-temperature solid oxide fuel cells (SOFCs). The alloy contains 20% to 24% chromium plus tungsten, niobium, titanium, and lanthanum. It has excellent corrosion resistance at temperatures to 900 C (1652 F), good electrical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (10): Ni-414.
Published: 01 October 1992
... Specilllell Type Alloy 622 sheet, unwelded Welded with Electrode 122 GTA welded with Filler Metal 622 Alloy 622 plate, unwelded Welded with Electrode 122 GMAc welded with Filler Metal 622 Alloy C-22 sheet, unwelded GTA welded with Filler Metal C-22 PROPERTIES Table 1 - TYPICAL MECHANICAL PROPERTIES (AS WELDED...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (7): Ni-407.
Published: 01 July 1992
...& unwelded Welded with Electrode 122 GTA welded with Filler Metal 622 Alloy 622 plate. nnwelded Welded with Ekmode 122 GMAC welded with Filler Meld 62.2 Alloy C-22 rhea. unwelded GTA welded with Filler MaalC-22 Boiling fenic sulfate. 5040 sulfuric B A t Ici l- c Test I m-h4 cQrror mm 46.1 48.8 i28A* ORate...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (3): Ni-624.
Published: 01 March 2005
.... Hastelloy and C-22 are trademarks of Haynes International, Inc. Nicrofer is a trademark of Thyssen Krupp VDM. Table 1 Typical Room Temperature Mechanical Properties of Inconel Alloy 22 Material thickness Tensile Yield strength, or diameter strength 0.2% offset Elongation, Hardness, Form mm in. MPa ksi MPa...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2009) 58 (3): SA-595.
Published: 01 March 2009
... 1.7380) ASTM II SA 387 gr.22 General Characteristics: CromElso 22 is a low-alloy Cr-Mo steel designed for pressure equipment such as hydrotreating reactors operating in hydrogen service in the temperature range up to 454 °C (850 °F). This alloy is manufactured via the electric arc furnace...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (3): Ni-559.
Published: 01 March 2000
... Properties: Elastic modulus at 22 °C (72 °F), GPa (106 psi) 207 (30.0) See also Table 1. Weldability: The AL 22 alloy is readily welded using gas tungsten arc weld- ing (GTAW), gas metal arc welding (GMAW), and shielded metal arc welding (SMAW) techniques. Filler metals are typi- cally made of matching...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (4): Cu-733.
Published: 01 April 2005
... MoldStar 18 has good bearing qualities and has resistance to wear, abrasion, fatigue, deformation, and corrosion. MoldStar 21 and 22 are harder alloys and also have good bearing qualities and resistance to wear, abrasion, fatigue, deformation, and corrosion. This family of aluminum bronzes is used...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (5): SS-903.
Published: 01 May 2004
... 40 Pipe butt weld 35 Impact toughness, J (ft lbf) 20 °C (68 °F), typical 60 73 (44 54) 20 °C ( 4 °F), typical 45 55 (33 41) 20 °C ( 4 °F), pipe butt weld 45 50 (33 37) 30 °C ( 22 °F), typical 40 52 (30 38) 30 °C ( 22 °F), pipe butt weld 42 46 (31 34) 30 °C ( 22 °F), heat treated >90 (>66) 1120...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (5): SS-926.
Published: 01 May 2005
... be joined by roll-seam welding. Corrosion Resistance: Crofer 22 APU is resistant to fuel cell anode gas and cathode gas at temperatures up to 900 °C (1652 °F). CROFER 22 APU Filing Code: SS-926 Stainless Steel May 2005 CROFER 22 APU (High-Temperature Alloy) Crofer 22 APU is an alloy especially developed...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (4): SS-1242.
Published: 01 April 2016
.... Cyclic Oxidation Resistance: This material has improved resistance to cyclic oxidation compared to the 17 18% chromium bearing alloys and superior performance when compared to Type 409. At 899 °C (1650 °F) this 22% chromium, low molybdenum ferritic alloy shows to have cyclic oxidation resistance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (2): Al-375.
Published: 01 February 2002
... consumption, lb/100 ft(c) 0.030 100 130 18 22 0.094 100 22 500 30 0.75 125 150 20 24 0.125 120 22 600 30 1 0.035 85 120 20 23 0.094 110 22 480 30 0.75 125 150 20 24 0.125 130 22 566 30 1 170 190 21 26 0.250 170 23 740 35 4 0.047 125 150 20 24 0.125 150 23 360 30 1 180 225 22 26 0.187 180 23 410 30 2.3 170 240...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2004) 53 (6): Ni-621.
Published: 01 June 2004
... ALLOY C-22HS (Corrosion-Resistant Nickel-Alloy) Hastelloy C-22HS has, like the other C-type alloys, excellent corrosion resistance, but it also exhibits high strength, nearly double the other alloys in the family. Hastelloy, C-22, and C-22HS are trademarks of Haynes International, Inc. 725...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2016) 65 (9): Al-446.
Published: 01 September 2016
...) Melting range, approximate, °C (°F) 624 646 (1155 1195) Anodize color White Mechanical Properties: Typical mechanical properties of GMAW groove joint welds (base alloy 5454-O) and typical ultimate tensile strengths at selected temperatures for GMAW groove joint welds (base 5454, filler 5554) are shown...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (9): Ni-322.
Published: 01 September 1985
... Carbon Columbium* Copper Nickel *Plus tantalum. Nominal 5.0 max. 29.5 5.0 2.5 15.0 1.0 max. 2.0 max. 0.03 max. 0.7 1.7 Remainder Physical Constants: Density, lb/cu in. (At 70°F) g/cu cm (At 22°C) Thermal coef. expansion/ F(86-400 F) (86-800°F) / (86-1200°F) C 30 204 C) (30-427 C) (30-649OC...