Alloy Digest (1972) 21 (10): SS-281.
Published: 01 October 1972
... ALLEGHENY LUDLUM OR-1 is a titanium-stabilized, ferritic chromium stainless steel with high resistance to oxidation. This datasheet provides information on composition, physical properties, and tensile properties as well as creep. It also includes information on high temperature performance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (11): SS-263.
Published: 01 November 1971
... ALLEGHENY LUDLUM MF-1 is a chromium-titanium corrosion resisting steel that was developed originally for automotive exhaust system applications. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (1): SS-360.
Published: 01 January 1979
... ALLEGHENY LUDLUM E-BRITE 26-1 ALLOY is a low-carbon, low-nitrogen ferritic stainless steel made by a vacuum refining process. It provides: (1) Excellent resistance to pitting and crevice corrosion in chloride-containing environments, (2) Excellent resistance to chloride stress-corrosion cracking...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (2): SA-560.
Published: 01 February 2007
... carbon steel would be. General Characteristics: For more than 30 years, the Washington Plant of Allegheny Ludlum Table 1 Bend Recommendations Condition Bend radius, × thickness, T Maximum load, lb Bend angle to crack Annealed 1T 2700 105° 2T 2620 180° Heat treated 2T 7740 (broke) 2° 4T 5760 (broke) 7° 6T...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2013) 62 (2): SS-1135.
Published: 01 February 2013
... ATI 409HP (UNS S40900) ferritic stainless steel was introduced by ATI Allegheny Ludlum to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon steel. The alloy was designated "MF-1", indicating its end use: automotive mufflers. The good...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (4): SS-270.
Published: 01 April 1972
... ALLEGHENY LUDLUM MF-2 is a 12% chromium steel that was developed initially for use in automobile exhaust systems. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on high temperature performance and corrosion resistance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1972) 21 (8): SS-277.
Published: 01 August 1972
... Ludlum 430F chemical composition corrosion-resistant alloys elasticity fatigue properties heat treatability high-temperature alloys joinability machinability physical properties tensile properties workability I 1 Filing Cock: ss-277 1 ALLEGHENY Umunm 430F 1 ~tainless~teel I I AUGUST 1972...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2001) 50 (11): SS-836.
Published: 01 November 2001
... Type 310L is similar to Allegheny Ludlum Type 310 (see Alloy Digest SS-719, June 1988) except that it has a very low carbon content. This change enhances corrosion resistance to strong oxidizing acids. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (1): SS-511.
Published: 01 January 1990
... International Allegheny Ludlum AL 904L alloy chemical composition corrosion-resistant alloys elasticity hardness heat treatability joinability machinability physical properties tensile properties workability UNS N08904 ALLEGHENY LUDLUM iilfsjf AL904LALLOY Filing Code: s-51 1 Stainless Steel...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
...: Plate is available in 316 1 4 in. thickness for 72 240 in. random lengths. For 3 8 in. and thicker plate, 96 × 300 in. is the maximum. A variety of plate shapes are available including abrasive cut bar. Producer: Allegheny Ludlum Corp. Pittsburgh, PA 15222-5479 (800) 258-3586 or (412) 394-2800 (724) 226...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (6): SS-470.
Published: 01 June 1986
... ALLEGHENY LUDLUM TYPE 439 is a stainless steel with a high resistance to chloride stress-corrosion cracking. It also has a high level of general resistance in steam and fresh-water environments. Its high level of chromium provides resistance to sulfidation and oxidation. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (1): Ni-366.
Published: 01 January 1989
... Allegheny Ludlum AL 825 alloy is a nickel-iron-chromium-molybdenum-copper alloy with superior corrosion resistance including stress-corrosion cracking resistance. It is highly ductile from cryogenic to well over 1000 F(538 C) temperatures. It is readily weldable. This datasheet provides...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1998) 47 (6): SS-719.
Published: 01 June 1998
... Allegheny Ludlum Type 310 is an austenitic chromium-nickel steel with high heat resisting properties. It is recommended for furnace equipment, heat treating boxes, burners, heat recovery systems, jet engine components, and heat exchangers. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (9): Ni-374.
Published: 01 September 1989
... Allegheny Ludlum AL 400 is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is not hardenable by heat treatment. It can be appreciably strengthened by cold work. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (3): Ni-559.
Published: 01 March 2000
... properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as joining. Filing Code: Ni-559. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 2000 2000 ASM International...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2007) 56 (10): SS-1000.
Published: 01 October 2007
... Allegheny Ludlum Type 201LN (AL 201LN) is a modification of Type 201 developed especially for cryogenic service to -195 deg C (-320 deg F) to handle industrial gases. Its strength and corrosion resistance also allow other applications. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (6): TS-288.
Published: 01 June 1975
... ALLEGHENY LUDLUM HTB-2 is a chromium-molybdenum-vanadium steel of the type commonly referred to as M-50. It is vacuum melted to meet cleanliness and rolling-contact-fatigue requirements of critical bearing applications for operating at elevated temperatures. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2000) 49 (11): Ti-115.
Published: 01 November 2000
... ratio of Allegheny Ludlum CP chemically pure Titanium alloys make them the materials of choice for many corrosive chemical environments, including oxidizing chloride solutions, seawater, and chlorine-based bleaches. Chemical Composition, wt R50250 R50400 R50550 R50700 UNS Grade 1 Grade 2 Grade 3 Grade 4...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (4): Fe-97.
Published: 01 April 1992
... Allegheny Ludlum No. 2 and No. 5 relay steels are iron/silicon alloys. They are soft magnetic alloys that combine high magnetic permeability, low residual magnetization and low coercive force with good mechanical properties and fabricability. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (1): Ni-497.
Published: 01 January 1996
... Allegheny Ludlum AL276 is widely used in the most severe environments found in chemical plants and in power plant desulfurization systems. The high molybdenum level with tungsten gives excellent pitting and crevice corrosion resistance. This datasheet provides information on composition, physical...