Alloy Digest (1956) 5 (10): SS-48.
Published: 01 October 1956
... ALLEGHENY LUDLUM 316 and 316L are acid resistant, molybdenum type 18-8 stainless steels. Type 316L is the low carbon grade of Type 316 offering decreased carbide precipitation. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity...
Journal Articles
Alloy Digest (2000) 49 (2): SS-776.
Published: 01 February 2000
... Allegheny Ludlum 316 and 316L are corrosion resistant, molybdenum bearing austenitic stainless steels. Type 316L is the low carbon grade of type 316 offering decreased carbide precipitation. The MINIMISER form is an improved machinability version with a change in the sulfur composition, still...
Journal Articles
Alloy Digest (2011) 60 (10): SS-1103.
Published: 01 October 2011
... resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1103. Producer or source: ATI Allegheny Ludlum Corporation. Producer or Source: ATI Allegheny Ludlum Corporation Copyright © ASM International® 2011 2011 ASM International ATI 50 Alloy chemical composition...
Journal Articles
Alloy Digest (1985) 34 (8): SS-462.
Published: 01 August 1985
... ALLEGHENY LUDLUM AL 2205 ALLOY is in the family of duplex alloys in which added nitrogen significantly improves corrosion resistance, especially in the welded condition. The microstructure consists of a balanced mixture of austenitic and ferritic phases. Its corrosion resistance to many...
Journal Articles
Alloy Digest (1986) 35 (6): SS-470.
Published: 01 June 1986
... ALLEGHENY LUDLUM TYPE 439 is a stainless steel with a high resistance to chloride stress-corrosion cracking. It also has a high level of general resistance in steam and fresh-water environments. Its high level of chromium provides resistance to sulfidation and oxidation. This datasheet provides...
Journal Articles
Alloy Digest (2015) 64 (5): SS-1207.
Published: 01 May 2015
..., and joining. Filing Code: SS-1207. Producer or source: Allegheny Ludlum. Producer or Source: Allegheny Ludlum Copyright © ASM International® 2015 2015 ASM International ATI 2102 chemical composition corrosion-resistant alloys hardness heat treatability high-temperature alloys joinability...
Journal Articles
Alloy Digest (2013) 62 (11): Fe-162.
Published: 01 November 2013
.... Producer or source: Allegheny Ludlum. Producer or Source: Allegheny Ludlum Copyright © ASM International® 2013 2013 ASM International ATI 9 chemical composition elasticity fracture toughness hardness heat treatability joinability physical properties tensile properties workability...
Journal Articles
Alloy Digest (1996) 45 (2): SS-639.
Published: 01 February 1996
... temperature performance and corrosion resistance as well as heat treating and joining. Filing Code: SS-639. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1996 1996 ASM International ALLEGHENY LUDLUM OHMALOY 30...