1-20 of 53 Search Results for

Allegheny Ludlum 316

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1956) 5 (10): SS-48.
Published: 01 October 1956
... ALLEGHENY LUDLUM 316 and 316L are acid resistant, molybdenum type 18-8 stainless steels. Type 316L is the low carbon grade of Type 316 offering decreased carbide precipitation. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity...
Journal Articles
Alloy Digest (2000) 49 (2): SS-776.
Published: 01 February 2000
... Allegheny Ludlum 316 and 316L are corrosion resistant, molybdenum bearing austenitic stainless steels. Type 316L is the low carbon grade of type 316 offering decreased carbide precipitation. The MINIMISER form is an improved machinability version with a change in the sulfur composition, still...
Journal Articles
Alloy Digest (1985) 34 (8): SS-462.
Published: 01 August 1985
.... Machinability: Allegheny Ludlum AL 2205 Alloy has good machining characteris:ics. When high-speed-steel tools are used, you may use the same cutting data that you would use for AISI Type 316. When machining with cemented-carbide tools. reduce cutting speeds 20% from those used for Type 316. Forming: AL 2205 can...
Journal Articles
Alloy Digest (1988) 37 (8): SS-497.
Published: 01 August 1988
... Allegheny Ludlum AL 17-4 Precipitation Hardening Alloy is a chromium-nickel-copper stainless steel. It maintains high strength to about 600 F (316 C) and it exhibits a moderate level of corrosion resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
.... AISI type 316 stainless steel filler metal has been used successfully to join alloy 255 to type 316 stainless steel. Corrosion Resistance: Typical corrosion resistance with ASTM G 28 Method A is 0.0010 in./month. ALLEGHENY LUDLUM ALLOY 255 Filing Code: SS-786 Stainless Steel 5/00; Corrected 6/02 Table...
Journal Articles
Alloy Digest (1978) 27 (4): SS-349.
Published: 01 April 1978
... data for ALdX and AISI Type 316. Weldability: Allegheny Ludlum AL-6X can be welded readily by the inert gas processes. Resistance to Corrosion and Oxidation: Allegheny Ludlum AL-6X is resistant to atmospheric corrosion and similar mild types of corrosion. In general, those media which have no corrosive...
Journal Articles
Alloy Digest (1989) 38 (1): Ni-366.
Published: 01 January 1989
... Allegheny Ludlum AL 825 alloy is a nickel-iron-chromium-molybdenum-copper alloy with superior corrosion resistance including stress-corrosion cracking resistance. It is highly ductile from cryogenic to well over 1000 F(538 C) temperatures. It is readily weldable. This datasheet provides...
Journal Articles
Alloy Digest (1990) 39 (1): SS-511.
Published: 01 January 1990
... ALLEGHENY LUDLUM AL 904L Alloy is an austenitic stainless steel designed for middle to high level corrosion resistance. It is produced to low carbon levels for use in the welded condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1986) 35 (6): SS-470.
Published: 01 June 1986
... advantage over AK1 Types 304 and 316. Joining: Type 439 tubes are easily connected with standard compression type fittings. Corrosion Resistance: ALLEGHENY LUDLUM TYPE 439 is resistant to attack by potable water and many mildly to moderately corrosive chemical environments which are neutral or oxidizing...
Journal Articles
Alloy Digest (1988) 37 (5): SS-494.
Published: 01 May 1988
... Allegheny Ludlum AL-6XN alloy is characterized as a superaustenitic stainless steel having an exceptional level of corrosion resistance, especially to chloride pitting. It has high strength and its impact value at room temperature is 140 ft-lb and at 320 F (196 C) is 85 ft-lb. It is covered...
Journal Articles
Alloy Digest (1989) 38 (4): Ni-370.
Published: 01 April 1989
... Allegheny Ludlum AL600 alloy is a nickel-chromium alloy designed for use from cryogenic up to 2000 F(1093 C) temperatures. Its nickel content provides resistance to reducing environments and stress-corrosion cracking. Its chromium affords resistance to mildly oxidizing conditions. It has excellent...
Journal Articles
Alloy Digest (1979) 28 (1): SS-360.
Published: 01 January 1979
... ALLEGHENY LUDLUM E-BRITE 26-1 ALLOY is a low-carbon, low-nitrogen ferritic stainless steel made by a vacuum refining process. It provides: (1) Excellent resistance to pitting and crevice corrosion in chloride-containing environments, (2) Excellent resistance to chloride stress-corrosion cracking...
Journal Articles
Alloy Digest (1996) 45 (1): Ni-497.
Published: 01 January 1996
... Allegheny Ludlum AL276 is widely used in the most severe environments found in chemical plants and in power plant desulfurization systems. The high molybdenum level with tungsten gives excellent pitting and crevice corrosion resistance. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2001) 50 (11): SS-836.
Published: 01 November 2001
... Type 310L is similar to Allegheny Ludlum Type 310 (see Alloy Digest SS-719, June 1988) except that it has a very low carbon content. This change enhances corrosion resistance to strong oxidizing acids. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1979) 28 (3): SS-362.
Published: 01 March 1979
... ALLEGHENY LUDLUM Type 29-4 is a low-interstitial ferritic stainless steel. It contains approximately 29% chromium and 4% molybdenum. The alloy provides excellent resistance to pitting, crevice corrosion, and stress-corrosion cracking in chloride-containing environments. Type 29-4 is used widely...
Journal Articles
Alloy Digest (1993) 42 (4): SS-542.
Published: 01 April 1993
... systems. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-542. Producer or source: Allegheny Ludlum Corporation. Producer...
Journal Articles
Alloy Digest (1989) 38 (9): Ni-374.
Published: 01 September 1989
... Allegheny Ludlum AL 400 is a ductile nickel-copper alloy with resistance to a variety of corrosive conditions. The alloy is not hardenable by heat treatment. It can be appreciably strengthened by cold work. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1998) 47 (5): SS-717.
Published: 01 May 1998
... resistance as well as forming, heat treating, and joining. Filing Code: SS-717. Producer or source: Allegheny Ludlum Corporation. Producer or Source: Allegheny Ludlum Corporation Copyright © ASM International® 1998 1998 ASM International ALLEGHENY LUDLUM AL 800H ALLEGHENY LUDLUM AL800AT...
Journal Articles
Alloy Digest (2011) 60 (10): SS-1103.
Published: 01 October 2011
... resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1103. Producer or source: ATI Allegheny Ludlum Corporation. Producer or Source: ATI Allegheny Ludlum Corporation Copyright © ASM International® 2011 2011 ASM International ATI 50 Alloy chemical composition...
Journal Articles
Alloy Digest (2000) 49 (11): SS-806.
Published: 01 November 2000
... Allegheny Ludlum Type 425 Mod is hardenable by heat treatment. This straight-chromium grade is used where strength, hardness and/or wear resistance need to be combined with corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile...