Alloy Digest (2003) 52 (1): Ni-600.
Published: 01 January 2003
... Allcorr (UNS N06110) is a single-phase, non-age-hardenable, nickel-base alloy for service in highly corrosive environments. It is characterized by outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress-corrosion cracking. The alloy...