1-3 of 3 Search Results for

Alkrothal 3

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2009) 58 (2): SS-1030.
Published: 01 February 2009
... Alkrothal 3 is a ferritic FeCrAl alloy that is recommended for use at temperatures up to 1000 deg C (1830 deg F). Typical applications are in rheostats and braking resistors. It is also used as electrical heating elements in industrial applications. This datasheet provides information...
Journal Articles
Alloy Digest (2013) 62 (2): SS-1136.
Published: 01 February 2013
... Alkrothal 720 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well...
Journal Articles
Alloy Digest (2009) 58 (3): SS-1032.
Published: 01 March 2009
... Alkrothal 14 is one of a family of ferritic FeCrAl alloys used in resistance wires. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low temperature performance as well as forming...