Alloy Digest (1969) 18 (8): Fe-38.
Published: 01 August 1969
... Alfenol is an unoriented 12% to 16% aluminum-iron alloy which has high electrical resistivity and low eddy current losses. It is furnished in the 12% aluminum and in the 16% aluminum grades. The recommended uses are for relays, gyro mechanisms, servo-mechanisms and toroid tape cores. This...