Skip Nav Destination
Close Modal
Search Results for
Alcoloy alloy 688
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-1 of 1 Search Results for
Alcoloy alloy 688
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Alloy Digest (1970) 19 (9): Cu-219.
Published: 01 September 1970
... ALCOLOY ALLOY 688 is a high-strength cobalt-aluminum modified brass alloy with good drawability and formability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information...
Abstract
View article
PDF
ALCOLOY ALLOY 688 is a high-strength cobalt-aluminum modified brass alloy with good drawability and formability. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-219. Producer or source: Olin Brass.