Alloy Digest (2020) 69 (2): Al-461.
Published: 01 February 2020
... Alcoa EZCast 370 is a heat-treatable, aluminum-silicon-magnesium-manganese high-pressure die casting (HPDC) alloy which is widely used for thin-walled, crash-resistant, structural components for automotive applications. This datasheet provides information on composition, physical properties...