Alloy Digest (1989) 38 (11): Al-232.
Published: 01 November 1989
... ALCOA 7475 was developed for sheet and plate applications that require high strength and a high level of guaranteed fracture toughness. It has the highest toughness for a given strength of the commercially available high-strength aircraft alloys. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2000) 49 (7): Al-371.
Published: 01 July 2000
... Alcoa alloy 2090-T83 is an aluminum-lithium sheet alloy with a combination of strength, low density, and corrosion resistance. The alloy is used in aerospace applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as...