Alloy Digest (2002) 51 (6): Al-378.
Published: 01 June 2002
... AlcoTec Weld Filler Wire 5556 is a non-heat-treatable wire with very high strength capabilities. The principal alloying elements are magnesium, manganese, chromium, and titanium. This datasheet provides information on composition, physical properties, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1992) 41 (9): Al-325.
Published: 01 September 1992
... ALCOTEC Filler Metal 5180 is a weld wire in the Al-Zn-Mg aluminum family that responds to post-weld thermal treatments. The wire is especially useful to match base-metal strengths in thin walls. This datasheet provides information on composition and tensile properties. It also includes information...