Alloy Digest (1954) 3 (9): Al-20.
Published: 01 September 1954
... ALCAN 135 is a heat treatable aluminum casting alloy having high strength, pressure tightness, and is capable of being cast in intricate shapes. It has high corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (2010) 59 (7): Al-430.
Published: 01 July 2010
... Alcan 6056 alloy is an Al-Si-Mg-Zn-Cu-Mn weldable alloy, developed to provide medium strength similar to the incumbent 2024 alloy, with a lower density. This datasheet covers Alcan 6056 in several tempers as fuselage bare sheets. The alloy posesses, in several tempers, a superior combination...
Journal Articles
Alloy Digest (2007) 56 (12): Al-408.
Published: 01 December 2007
... Alcan 6156 T4, T6 clad sheets were developed with weldability and high damage tolerance compared with incumbent 2024 alloy. Aerospace applications include fuselages clad sheets. This datasheet provides information on composition, physical properties, and tensile properties as well as fatigue...
Journal Articles
Alloy Digest (1956) 5 (7): Al-41.
Published: 01 July 1956
... ALCAN 26S is a wrought heat treatable aluminum alloy recommended for structural applications requiring high strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1969) 18 (3): Al-185.
Published: 01 March 1969
.... PeMwlVZa Ie Kaiser Aluminum &Chemical Co., Oakland. Cabfomra Alcan lndustnes L&i.. Banbury. EngJmd Aluminum Co. ofCanada L,d.. Monueal. Canada Radii for various ThkktK~s (I) Temper I/64 1132 l/16 I/s 3116 l/4 318 I I? -- TO 0 0 0 011 1.2, I &31 241 A 4-61 zii IYI-3, 3-5, 2: 5-7, Sk-81 Ti I-2, I %3...