1-11 of 11 Search Results for

Al-SiC

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2012) 61 (1): Al-438.
Published: 01 January 2012
... Al-SiC is a 68% volume fraction alpha-silicon carbide aluminum alloy. Al-SiC materials provide superior thermal management for high technology electronics applications in a lightweight, cost-effective material. This datasheet provides information on composition, physical properties, microstructure...
Journal Articles
Alloy Digest (1999) 48 (2): Al-359.
Published: 01 February 1999
...-Matrix Composite) 6092/SiC/17.5P is a discontinuous metal-matrix composite fully characterized for discontinuously reinforced alloy (DRA) structural applications. The base al- loy is Aluminum Association 6092, and the reinforcement material is SiC. Chemical Composition, wt Physical Properties: (T6 temper...
Journal Articles
Alloy Digest (1995) 44 (1): Al-331.
Published: 01 January 1995
... DURALCAN F3D is a general purpose die casting composite with a matrix alloy similar to 380 (See Alloy Digest Al-239, July 1982). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (1995) 44 (2): Al-332.
Published: 01 February 1995
... DURALCAN F3N.xxS is an aluminum composite with virtually no Cu or Ni designed for use in corrosion-sensitive applications. The matrix alloy is similar to 360 (See Alloy Digest Al-103, May 1961, and Al-245, April 1983). This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1997) 46 (10): Al-342.
Published: 01 October 1997
... counterpart It is available as sand castings with a T6 heat neatment LanxideandPlimexcastare- of Lauxide Corporation; U.S. and foreign patents issued and pending. Chemical Composition: Matrix (10 Al-lSi-Mg), vol.8 Reinforcement (Sic particulate), voL% Physical Properties: 70 30 Density @tlk) at 21 OC (7ooF g...
Journal Articles
Alloy Digest (1994) 43 (10): Al-329.
Published: 01 October 1994
... Duralcan F3S.xxS is a heat treatable aluminum alloy-matrix gravity composite. The base alloy is similar to Aluminum 359 (Alloy Digest Al-188, July 1969); the discontinuously reinforced composite is silicon carbide. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1994) 43 (11): Al-330.
Published: 01 November 1994
... provides information on composition, physical properties, and tensile properties as well as creep. Filing Code: AL-330. Producer or source: Alcan Aluminum Corporation. Producer or Source: Alcan Aluminum Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition...
Journal Articles
Alloy Digest (1957) 6 (10): Al-57.
Published: 01 October 1957
... on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-57. Producer or source: Imperial Chemical Industries Inc.. Producer or Source: Imperial Chemical Industries Inc. Copyright © ASM International® 1996 1996 ASM...
Journal Articles
Alloy Digest (1992) 41 (8): SS-533.
Published: 01 August 1992
... 7.862 See Table 1 28.1 x 106 193 x 10 1.011 1.011 1.014 1.015 Table 1 - COEFFICIENT OF THERMAL EXPANSION, LINEAR F ( C) AL/L/ Fx@ AL/L/T x lOA 72-200 (22-93) 8.98 16.2 72400 (22-204) 8.96 16.1 72-600 (22-3 16) 9.60 17.3 72-800 (22427) 10.19 18.3 72-1000 (22-538) 10.46 18.8 Table 3 - EFFECT OF COLD...
Journal Articles
Alloy Digest (1971) 20 (3): CS-19.
Published: 01 March 1971
... of Cut 0.010 in. 0.050 In. 0.100 in. Tool Speed Feed Speed Feed Speed Feed Steel Material fpm ipr fpm ipr fpm ipr Fremax 15 High Speed Steel 160 0.005 150 0.007 145 0.010 AISI 1020 High Speed Steel 120 0.005 115 0.007 110 0.010 Fremax 15 Brazed Carbide 600 0.006 570 0.010 540 0.015 Al.9 1020 Brazed...
Journal Articles
Alloy Digest (1998) 47 (10): Ti-105.
Published: 01 October 1998
... TIMETAL 21S (Ti-15%Mo-3%Nb-3%Al-0.2Si) offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aerospace applications include engine exhaust plug and nozzle assemblies. This datasheet provides information...