Alloy Digest (1972) 21 (6): SA-275.
Published: 01 June 1972
... AWHF STEEL is a high-formability steel produced regularly at minimum yield strengths of 45,000 and 50,000 psi and for special applications at 55,000 and 60,000 psi. It is recommended for difficult cold-forming applications that involve bending or drawing and it has good weldability. This datasheet...