Alloy Digest (2001) 50 (10): SS-501.
Published: 01 October 2001
... Avesta Polarit 724L is a 17-13-2.5L special austenitic stainless steel developed for use in urea production, especially hot carbamate solutions. The alloy also has a very high resistance to intergranular corrosion. This datasheet provides information on composition, physical properties, hardness...