Alloy Digest (1993) 42 (10): SS-552.
Published: 01 October 1993
... AVESTA 654 SMO is an austenitic stainless steel which due to its high content of molybdenum and nitrogen possesses excellent resistance to pitting and crevice corrosion. It also has very high resistance to general corrosion in acids, especially those containing halide ions. Furthermore, its...
Journal Articles
Alloy Digest (2001) 50 (7): SS-465.
Published: 01 July 2001
... significantly stron- ger than most low-carbon stainless steels and its structural stability makes for good weldability. AvestaPolarit, 254 SMO, 654 SMO, and 2205 Code Plus Two are registered trademarks of AvestaPolarit AB. SAF 2304 and SAF 2507 are trademarks of AB Sandvik Steel. Chemical Composition, wt Carbon...