1-20 of 36 Search Results for

ATI 80 A

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2021) 70 (2): Ni-767.
Published: 01 February 2021
... ATI 80 A is a wrought, precipitation-hardenable, Ni-Cr-Ti-Al alloy that is generally used for high strength applications up to 760 °C (1400 °F), but may also be used at temperatures up to 845 °C (1550 °F) for short duration service. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2020) 69 (2): Ti-163.
Published: 01 February 2020
... MPa ksi MPa ksi % % 1 R50250 240 35 138 20 24 30 2 R50400 345 50 275 40 20 30 3 R50550 450 65 380 55 18 30 4 R50700 550 80 483 70 15 25 (a) Product diameter or thickness 75 mm (3 in (b) For information only (Source: ATI). Source: ATI, ASTM F67:2013(2017) and ISO 5832-2:2018 Hardness(b), max HRBW 70...
Journal Articles
Alloy Digest (2022) 71 (5): SS-1347.
Published: 01 May 2022
... ATI 201LN is an austenitic stainless steel that was specifically created for sub-zero temperature service down to –196 °C (–320 °F). It has replaced the familiar 300 series austenitic stainless steels such as type 301 and type 304 in many applications based upon technical equivalency and economic...
Journal Articles
Alloy Digest (2013) 62 (11): Fe-162.
Published: 01 November 2013
... ATI 9 is a nonmagnetic, modified Hadfield steel, austenitic. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and joining. Filing Code: Fe-162...
Journal Articles
Alloy Digest (2013) 62 (1): SS-1131.
Published: 01 January 2013
... ATI 444 is a low-carbon and low-nitrogen ferritic stainless steel with 18Cr and 2Mo and is often referred to as "18-2". This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2020) 69 (1): Ti-162.
Published: 01 January 2020
... ATI corrosion-resistant commercially pure (CP) titanium represents a family of unalloyed (Grades 1, 2, 3 and 4) and palladium alloyed (Grades 7, 11, 16 and 17) CP titanium that is produced as plate, sheet and strip. It is the material of choice for many corrosive chemical environments, including...
Journal Articles
Alloy Digest (2023) 72 (1): Ti-188.
Published: 01 January 2023
... to above 40 m/s (130 fps). Hydrogen Embrittlement. ATI CP Grade 17 Titanium is susceptible to hydrogen embrittlement under some circumstances. Absorption of hydrogen normally occurs when the temperature is above 80 °C (175 °F), and the ATI CP Grade 17 Table 1 Room temperature tensile properties...
Journal Articles
Alloy Digest (2017) 66 (2): SS-1258.
Published: 01 February 2017
... Product Room temperature tensile properties Ultimate strength, MPa (ksi) 0.2% yield strength, MPa (ksi) Elongation in 50 mm (2.0 in % Hardness, BHN Hardness, HRC Sheet/strip 4.75 mm ( 0.187 in.) Minimum for S322003 per ASTM A240 689 (100) 483 (70) 25 293 31 Typical of ATI 2003 LDSS 758 (110) 552 (80...
Journal Articles
Alloy Digest (2021) 70 (6): Ti-179.
Published: 01 June 2021
... of hydrogen normally occurs when the ASTM B265:2020 Ti2Pd (3.7235) temperature is above 80 °C (175 °F) and ATI CP Grade 11 DIN 17851:1990 Titanium is galvanically coupled to an active metal or an DIN 17860:2010 Class 11 impressed current or the pH is less than 3 or greater than 12. JIS H 4600:2012 Hot Forming...
Journal Articles
Alloy Digest (2021) 70 (9): Ti-182.
Published: 01 September 2021
... Titanium Hydrogen Embrittlement. ATI CP Grade 16 Titanium is sus- Grade 16 (UNS R52402) ceptible to hydrogen embrittlement under some circum- ATI stances. Absorption of hydrogen normally occurs when the ASTM B265:2020a Class 18 temperature is above 80 °C (175 °F) and the ATI CP Grade JIS H 4600:2012 Grade...
Journal Articles
Alloy Digest (2021) 70 (2): Ti-175.
Published: 01 February 2021
... Titanium is sus- ceptible to hydrogen embrittlement under some circum- Low density; high strength-to-weight ratio; moderate stances. Absorption of hydrogen normally occurs when the strength; high ductility; high toughness; excellent corrosion temperature is above 80 °C (175 °F) and when ATI CP Grade...
Journal Articles
Alloy Digest (2009) 58 (9): SA-606.
Published: 01 September 2009
... ATI 500-MIL High Hard is a specialty steel of wrought Ni-Cr-Mo specialty steel for armor plate. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining...
Journal Articles
Alloy Digest (2009) 58 (7): Ni-671.
Published: 01 July 2009
... with a strong contribution from cobalt. This age-hardened alloy has superior strength with oxidation resistance to 1095 °C (2000 °F) and is used on all forms of turbines. Allvac and Nickelvac are registered trademarks of ATI Properties, Inc. Chemical Composition, wt Min Max Nickel bal Cobalt 19.0 21.0 Chromium...
Journal Articles
Alloy Digest (2007) 56 (5): Ni-649.
Published: 01 May 2007
... and creep properties at temperatures up to 815 °C (1500 °F) after suitable heat treatment. The alloy has oxidation resistance up to 980 °C (1800 °F). It is typically used in aircraft turbine and structural components. Altemp is a registered trademark of ATI Properties, Inc. Mechanical Properties: Modulus...
Journal Articles
Alloy Digest (2021) 70 (11): Ti-184.
Published: 01 November 2021
...- excellent resistance to stress-corrosion cracking in hot chlo- ing, electron beam welding, and diffusion bonding can ride salt solutions. also be used. Information on heat treatment sourced from Corrosion-Resistant Titanium: Commercially Pure, ATI, 2013. Erosion Corrosion. Bibus Metals Titan Grade 1...
Journal Articles
Alloy Digest (2006) 55 (7): Ti-139.
Published: 01 July 2006
... as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-139. Producer or source: ATI Allvac. Producer or Source: ATI Allvac Copyright © ASM International® 2006 2006 ASM International ALLVAC Titanium-6Aluminum...
Journal Articles
Alloy Digest (2005) 54 (9): W-28.
Published: 01 September 2005
... to radiation shielding. Densalloy is a trademark of ATI Industries. DOI: 10.31399/asm.ad.w0028 Applications: SD 170 is widely used for ballast and counterbalance weights, inertial damping, and radiation shielding applications. SD 175 has general-purpose applications including chatter-free toolholders, rigid...
Journal Articles
Alloy Digest (2020) 69 (3): SS-1316.
Published: 01 March 2020
... °F) 100 °C (212 °F) 0 100 °C (32 212 °F) 21 °C (70 °F) Source: Sandmeyer Steel Company, AK Steel, and ATI Value 1482 1532 (2700 2790) 7750 (0.280) 10.8 (6.0) 12.6 (7.0) 24.9 (14.4) 460 (0.11) 0.57 (344) Mechanical Properties Tensile Properties and Hardness 0.2% proof strength Tensile strength MPa ksi...
Journal Articles
Alloy Digest (2020) 69 (12): Ti-173.
Published: 01 December 2020
... to its low modulus of elasticity and high yield strength, it exhibits a high degree of springback in cold forming. Cold forming information sourced from Zapp AG and ATI. Heat Treatment Heating. Heating should preferably be performed in an inert gas atmosphere or in vacuum. Annealing. Heat to about 730 °C...
Journal Articles
Alloy Digest (1982) 31 (10): Cu-446.
Published: 01 October 1982
... 1980, Engineering Pubkotions. Inc. Ati rights fe5mvd. -by . . JMP-%MqrsDigaSI= ISSN: 002-614X PostotTiceBon8p3 Uppes Mane, New jersey Copper Alloy No. C842tW (Cast Leaded Semi-Red Brass1 Copper Alloy No. C84200 is a free-cutting copper-zinc-tin-lead alloy. It is characterized by good casting properties...