Alloy Digest (2020) 69 (12): Ni-765.
Published: 01 December 2020
... ATI 6230 is a solid-solution strengthened, corrosion and heat-resistant, Ni-Cr-W-Mo-Al-La alloy. It is typically used for parts requiring good resistance to oxidizing environments up to 1150 °C (2100 °F) and relatively high strength up to 980 °C (1800 °F); however, usage is not limited...